glass crucible

I have always purchased my 200lb pots from engineered ceramics in north Illinois. I can not seem to find them are they out of business.
Reply With Quote
  #2  
Old 11-05-2017, 12:36 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 198
David Russell is on a distinguished road
My 200# crucible from hi temp/Pete has preformed every bit as good as the old ones from E.C. maybe better.
Reply With Quote
  #3  
Old 11-05-2017, 12:46 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,672
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by George Tessman View Post
I have always purchased my 200lb pots from engineered ceramics in north Illinois. I can not seem to find them are they out of business.
*******
Where are you looking for them? Selee Corporation is the holding company of EC and Selee bought EC for only one reason and that was a ceramic filter for another firm they also hold. A strange purchase.
As to quality, there are people who swear at, or swear by every manufacturer of crucibles out there. I repped both companies and did the mold designs for both as well. I'd just as soon not get into who is better than who. They all do different things depending on differing needs.

You could try googling Selee Corp.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 11-05-2017, 02:14 PM
George Tessman George Tessman is offline
Registered User
 
Join Date: Jun 2004
Location: Highland, IN
Posts: 233
George Tessman is on a distinguished road
Thank you . I was purchasing from them because they were within driving distance for me . So no shipping costs. I get about three years out of the crucible . And that's with batching
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:45 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.