Chalcedony, Silver Opal

I melted a new color this week. It looks pretty good but I would like a little more red tone to it. It is a dark amber in transmitted light. Recipe for 100 pounds Spruce Pine Color Base
300 gm zinc oxide
280 gm black tin
46 gm silver nitrate
20 gm red iron oxide
melted at 2125, taken up to 2260 7 hours after last charge.
Fairly seedy first day, fewer very small seeds second day.

Should I use a little less red iron or less silver nitrate?
Attached Images
File Type: jpg silverOpalw..jpg (25.3 KB, 98 views)
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:37 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.