Quote:
Originally posted by Mike Crowley
i have a 80 lb pot on ely's 13 gage kantholl 10 inch's of insulation.
i melt eltromelt, cook for 8 hours at 2280 squeeze for 4 hours , no bubs or cords just nice glass. so far the 13 gage are on there 6th week the 14 gage i was using only lasted 3 weeks .

mike
how long do you get on a set of elements? what yield do you get (lbs batch vs. lbs glass)?
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 10:37 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2023, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.