Revisit Air gas mix for glory hole

Every so often I look at my glory hole and admire the most inefficient furnace .
So much heat is lost through the door. But that is another story.
I never found a way to determine the adjustments for the best air gas mixture.
I look for a blue flame and a guttural growling sound.
I remember someone talking about making the flames come outside the door.
Then after heat up dial back the gas to make the flame go back inside.
I tried it yesterday and instead of dialing back the gas I dialed back the air to make the flame come out the door.
Is it the best mixture when the flame comes out the door?
Franklin
Reply With Quote
  #2  
Old 12-10-2018, 11:38 PM
Nick Delmatto Nick Delmatto is offline
Registered User
 
Join Date: Feb 2010
Location: Logan, OH
Posts: 44
Nick Delmatto is on a distinguished road
Yes, but not too much. Observe & adjust.
Reply With Quote
  #3  
Old 12-11-2018, 07:15 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,480
Eben Horton is on a distinguished road
You are doing it right franklin.
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 12-11-2018, 11:07 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is online now
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,821
Franklin Sankar is on a distinguished road
Thanks . Do you have the small flames coming out of the door all the time or only at startup.
Franklin
Reply With Quote
  #5  
Old 12-11-2018, 12:47 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,480
Eben Horton is on a distinguished road
When I start working I fine tune the hole so that the little flames just barely go away. To tune it right you use your eyes and ears. The little flames will turn silver colors silver which can be nice
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 12-12-2018, 04:56 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is online now
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,821
Franklin Sankar is on a distinguished road
I hope it donít turn my crystal looking glass dirty looking. FHC
Franklin
Reply With Quote
  #7  
Old 12-13-2018, 06:01 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 924
Sky Campbell is on a distinguished road
Fenton heavy crystal (FHC) sounds like it would have lead in it but it does not. It is a simple soda lime glass so reduction should not turn it grey.



I always felt flames licking out of the hole implies incomplete combustion. The gas is combusting outside of the glory hole. The flames are a good indicator before you dial the air up or the gas down. It does help you tune it in but any flames outside the hole aren't doing anything but heating the shop.
Reply With Quote
  #8  
Old 12-14-2018, 07:51 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,963
Pete VanderLaan is on a distinguished road
Excessive antimony in a clear glass will cause it to grey up on the surface in heavy reduction. Really excessive antimony makes an opaque.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 12-16-2018, 08:40 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is online now
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,821
Franklin Sankar is on a distinguished road
Thanks. It also seems that The excess flames also waste the gas.
Now to prevent the graying.
Franklin
Reply With Quote
  #10  
Old 12-17-2018, 07:59 PM
Jordan Kube Jordan Kube is online now
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,673
Jordan Kube is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
Fenton heavy crystal (FHC) sounds like it would have lead in it but it does not. It is a simple soda lime glass so reduction should not turn it grey.



I always felt flames licking out of the hole implies incomplete combustion. The gas is combusting outside of the glory hole. The flames are a good indicator before you dial the air up or the gas down. It does help you tune it in but any flames outside the hole aren't doing anything but heating the shop.
Depends on the geometry of your glory hole, etc. Depending on how hot you want the gloryhole you may not get there without a "stinger" popping out the front. Usually it's a fast short type of flame that is composed of well mixed hot gasses. It just won't all fit in there. Lazy flames are rich flames.
__________________
WWUD? Think for yourself.
Reply With Quote
  #11  
Old 12-18-2018, 01:47 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is online now
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,821
Franklin Sankar is on a distinguished road
Sometimes I get it very hot but sometimes it is so lazy it just relaxes at a lower temperatre. Yes the hot I want is when the flame licks out a bit . Is that a stinger? When I open up the air the flame seem to be colder and does not come out. I find the best way to get the flame to come out o is to cutback the air.
Franklin.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:39 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.