Has anyone used cane and murrine made with bomma with SP87 wer? Any info would be great. I have used SP and crystalica with out any problems but never bomma. I am always curious other peoples experience.
Thanks
Aron
Reply With Quote
  #2  
Old 04-29-2020, 06:17 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,734
Eben Horton is on a distinguished road
You should be fine !
__________________
<eben epoiese>
Reply With Quote
  #3  
Old 04-29-2020, 06:56 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 695
Josh Bernbaum is on a distinguished road
To be safe, do a test by incorporating some of the two (Bomma murrini and SP) in the same small piece. Then try to saw through it with a wet saw after annealing. See what happens. If it saws cleanly, then great, but if not, then no bueno. What color(s) are in the cane could be an additional variable.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:28 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.