Cast iron shaping blocks

Cast Iron shaping blocks> I have 9 of these a couple larger and smaller. 30.00 each. Can send pictures if you give me your email.
Attached Images
File Type: jpg shaping blocks_edited-1.jpg (59.4 KB, 88 views)
Reply With Quote
  #2  
Old 11-28-2018, 09:37 AM
Bill Worcester Bill Worcester is offline
Registered User
 
Join Date: Apr 2009
Location: Maui, HI
Posts: 55
Bill Worcester is on a distinguished road
Please send photos

Gosparky@hawaii.rr.com
Thanks, ,Bill
Reply With Quote
  #3  
Old 12-01-2018, 08:15 PM
bob gent bob gent is offline
Registered User
 
Join Date: Oct 2016
Location: lawrence, ks
Posts: 9
bob gent is on a distinguished road
bob@bobgent.com
I want one of the large ones, please
Reply With Quote
  #4  
Old 12-03-2018, 04:33 PM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,140
Scott Novota is on a distinguished road
I think I would like to try out one of these guys. If they don't work out I will gift them to the local art center.

scott - AT- novota -dot- come
Reply With Quote
  #5  
Old 12-03-2018, 06:20 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,012
Pete VanderLaan is on a distinguished road
We had those things in Shanghai and I never got excited about them. What I do periodically use is old crucibles, broken up and laid on their sides with newsprint in them. That really gives some nice shapes if you're blowing into them.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 12-04-2018, 05:46 PM
James Burts James Burts is offline
Registered User
 
Join Date: Jul 2014
Location: Raleigh, NC
Posts: 39
James Burts is on a distinguished road
I've just recently started experimenting on using one of these, and would be interested in seeing the different sizes you have available. Could you send pictures to jburts at gmail?
Reply With Quote
  #7  
Old 12-05-2018, 09:06 AM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 102
Eric Trulson is on a distinguished road
I'd be interested in trying out one or two of these. Email is: eric[at]trulsondesign[dot]com
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:28 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.