Nikon (Hikari) Glass used for lenses.

Maybe a bit OT but this article was interesting. Especially that IoR can be controlled through annealing.

https://www.imaging-resource.com/new...-glass-factory
Reply With Quote
  #2  
Old 04-01-2019, 12:45 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 920
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Brian Wong Shui View Post
Maybe a bit OT but this article was interesting. Especially that IoR can be controlled through annealing.

https://www.imaging-resource.com/new...-glass-factory
Wow that was really a great article. Thanks for sharing, I found it fascinating.
Reply With Quote
  #3  
Old 04-01-2019, 04:44 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 97
Eric Trulson is on a distinguished road
Thank you for sharing, that was a pleasantly detailed overview of some technically impressive glass melting. Wild how they need to account for the extra silica dissolved into the melt from the pot wall, and the additional loss of volatiles near the center of the pot.

I would sign a "take-my-firstborn-and-my-right-hand-if-I-ever-tell-anyone-anything" level of nondisclosure agreement for a chance to actually check out their final melting furnace though (the one that remelts the frit from the primary melter and casts the continuous bar of optical quality glass). Super curious what technical hoops they need to jump through to maintain glass quality during that stage of the process.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:13 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.