Spruce pine "Everclear" batch. TS replacement.

Hello. I'm wondering if anyone has any experience with the new "Everclear" batch from Spruce Pine? I called to order there 87 Texas Sand but was told they have replaced that formula with a new "clearer" batch. I ordered it because,hell, its Spruce Pine batch so I trust it.

Just curious if anyone has any experience or knowledge that could be shared.

Thanks
Reply With Quote
  #2  
Old 04-09-2019, 03:53 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,956
Pete VanderLaan is on a distinguished road
the new silica is phenomenal.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 04-09-2019, 03:57 PM
Philip Yamron Philip Yamron is offline
Registered User
 
Join Date: Jul 2012
Location: Ann Arbor, MI
Posts: 66
Philip Yamron is on a distinguished road
Great!!

What makes you feel that way?
Reply With Quote
  #4  
Old 04-09-2019, 04:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,956
Pete VanderLaan is on a distinguished road
The results. I get to see this stuff. While I won't go into sourcing, I will say that the processing of the material was critical to the success. Greg and I were talking about this stuff almost a year ago. I'm not at liberty to say why it worked, but with some interesting technology it's great. I'll have my next pallet of it made this way and I'm already really happy with the clarity now.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 04-10-2019, 01:31 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,477
Eben Horton is on a distinguished road
I use it. Itís amazingly clear. Zero shades of green.
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 04-10-2019, 01:47 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,042
Greg Vriethoff is on a distinguished road
Will this be available in Snowflake?
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #7  
Old 04-10-2019, 01:59 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,477
Eben Horton is on a distinguished road
Yes...........
__________________
<eben epoiese>
Reply With Quote
  #8  
Old 04-10-2019, 07:04 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,042
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Yes...........
Awesome! Thank you.
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #9  
Old 04-11-2019, 07:15 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,956
Pete VanderLaan is on a distinguished road
Everything is available in snowflake. That's simply a question of the amount of water in the mix.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 04-11-2019, 03:03 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,042
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Everything is available in snowflake. That's simply a question of the amount of water in the mix.
What's the minimum for an order?
__________________
"Technique is just a means of arriving at a statement." - Jackson Pollack
Reply With Quote
  #11  
Old 04-11-2019, 03:09 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,956
Pete VanderLaan is on a distinguished road
I'm not a sales rep. You need to ask Candy. For my batch, it's one ton and it's a better glass if that matters. Both are dead on 96. It does seem to me that the price is the same for the everclear as opposed to the texas sand.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 04-11-2019, 09:13 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,477
Eben Horton is on a distinguished road
Everclear is the new Texas sand, Pete. New sand. New name.
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:18 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.