Unwinding part of coil

I used a long nose pliers and wrapped the tip with tape and used it to help unwind a heater coil so I can pass the straight part between rows and continue the coil in the next row. The coil is very stiff and my fingers are not that strong.
Anyone has some tricks they use to make the unwinding easier. 3/8 inches diameter coil.
Franklin.
Attached Images
File Type: jpg image.jpg (56.4 KB, 33 views)
Reply With Quote
  #2  
Old 05-08-2019, 11:36 AM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 585
Shawn Everette is on a distinguished road
Is that an unfired coil? If so it should have be effectively "annealed" and fairly soft. A light hold in a vice might help if grip strength is an issue.
Reply With Quote
  #3  
Old 05-08-2019, 02:07 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,971
Franklin Sankar is on a distinguished road
Yes itís unfired but not as easy to do what I am doing. I am using 1 long coil instead of 1 coil in each row. So I have to unwind the coil to get from one row to the next.

Next time it will be different. 1 coil per row.
I nicked the surface of the wire and even though itís a small nick it is a good place for failure.
Thanks
Franklin
Reply With Quote
  #4  
Old 05-08-2019, 02:50 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 585
Shawn Everette is on a distinguished road
Alternatively if you had vertical area routed from row to row you wouldn't need to undo the coil. The nick will be a likely failure point, changes in diameter is going to make changes in resistance.
Reply With Quote
  #5  
Old 05-08-2019, 06:52 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,971
Franklin Sankar is on a distinguished road
Thanks. If I could join the wires it would extend the life. Maybe I could use a welding torch and see if it can melt the wire to mend the nick. But then that may change the chemistry of the wire and create a weak spot.
Time to get read now for the next failure.
Franklin
Reply With Quote
  #6  
Old 05-09-2019, 05:45 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 635
Peter Bowles is on a distinguished road
Hi Franklin,
Try heating the area to be straightened with a map gas torch or similar - heat to a moderate orange heat and then as the wire is still hot gently pull and untwist the coil from both sides. The emphasis is on the untwist rather than the pulling.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:42 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.