I love Bomma very much but I do a lot of spot-torching and find Bomma is very sensitive to reducing. I use a Bernzomatic torch with MAPP gas. Has anyone used a good torch with oxy-gas or oxy-propane on Bomma and how is that working out?
Reply With Quote
  #2  
Old 12-06-2019, 05:07 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 520
Shawn Everette is on a distinguished road
Ditto. Hot torch doesn't "reduce", but there is a surface change. Sometimes you can see it if you're just finishing up a piece, but if you keep working it goes away.
Reply With Quote
  #3  
Old 12-06-2019, 05:12 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,717
Pete VanderLaan is on a distinguished road
Likely caused by antimony in the glass which doesn't exactly Brown up, but it does discolor. One of the things about torching is to avoid having the valence switch in the antimony from penta to mono valent as it suddenly gets a lot hotter. I think Shawn could be more expansive about how his fix works, and why.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 12-07-2019, 10:12 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 520
Shawn Everette is on a distinguished road
If you're trying to torch a punty mark it shows, but if you manage to get it floppy again it goes away. Same if you gather over it. Don't have a why for you.
Reply With Quote
  #5  
Old 12-06-2019, 05:54 PM
David Patchen's Avatar
David Patchen David Patchen is online now
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,906
David Patchen is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Ditto. Hot torch doesn't "reduce", but there is a surface change. Sometimes you can see it if you're just finishing up a piece, but if you keep working it goes away.
I have found the same thing--Bomma doesn't love a super-hot flame. I thought the brown was burning the glass a bit. I've backed off the gas mix in my hot torch and that helps a lot.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:23 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.