Coppe, gold, silver foil

What are some techniques when using metal foils?
Reply With Quote
  #2  
Old 10-07-2019, 09:46 PM
Marty Kremer Marty Kremer is online now
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 482
Marty Kremer is on a distinguished road
Quote:
Originally Posted by Art Ciccotti View Post
What are some techniques when using metal foils?
For what??
Reply With Quote
  #3  
Old 10-08-2019, 10:48 AM
Art Ciccotti Art Ciccotti is offline
Registered User
 
Join Date: Dec 2008
Location: Ames,Iowa
Posts: 72
Art Ciccotti is on a distinguished road
Foil

Sorry not being specific. I want to use the foil as a surface decoration on the outside of vases, paperweights.
Reply With Quote
  #4  
Old 10-08-2019, 12:55 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 507
Shawn Everette is on a distinguished road
Paperweights will generically be fine, but foil on blown can be funky. It can make things stiff an blow out weird. Leaf works a little better, but disappears easy when stretched. Copper can be difficult to get the nice reds without burning out, silver and gold are pretty straight forward. Vacuum tables make things much easier. I'm sure it costs a small fortune, but Rik Allen does an application by hand on the exterior of his rockets that is freaking gorgeous.
Reply With Quote
  #5  
Old 10-08-2019, 04:52 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 768
Michael Ahlefeldt-Laurvig is on a distinguished road
Art, really, you shouldnt ask that here, if you blow glass it doesent make sense

Last edited by Michael Ahlefeldt-Laurvig; 10-08-2019 at 04:57 PM.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:55 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.