208V-3 Phase / 240V-1 Phase Kilns (Revisisited)

I've read through some of the past postings, and still have a few questions:

I have at my shop only 208V Three Phase power. I have a couple of casting kilns that are rated for 240V Single Phase at 45 Amps. Has anyone had any actual experience using a kiln like this:

1: As-is, on 208V If so, how much more time does it take to get to temperature? Do you have to reprogram the controller? Do you need to open the controller, and rewire the controller on it's separate 120V power?

2. Anyone have a good experience using a Buck Transformer in this situation? If so teach me please!

3. Anyone here remove the elements, cut them down for 208V?

Thanks!
Reply With Quote
  #2  
Old 08-27-2018, 06:17 PM
Jordan Kube Jordan Kube is online now
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,650
Jordan Kube is on a distinguished road
1. If you plug it right into 208 you'll only be getting 75% of the power you had with 240v. Only you will be able to guess how long it will take. You haven't provided any construction data for the kiln. You should not need to reprogram the controller. Most controllers will accept 120-240v AC power inputs but you will need to check the controller specs. Some run on DC.

2. and 3. Best to just get a new set of elements rewound to your voltage.

If your elements are in sets of threes you can use the 3 phase, which is a different set of calculations, otherwise, you can pull 208 single phase out of the panel. If you don't have someone to help the latter option might be easiest.
__________________
WWUD? Think for yourself.
Reply With Quote
  #3  
Old 08-28-2018, 09:48 AM
Rick Wilton Rick Wilton is offline
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 190
Rick Wilton is on a distinguished road
I had to add an extra element to my big kiln when I moved it into a shop with 3 phase 208v power. It would still get to top temp but was just too slow for my liking. I was getting devit issues when fusing some projects. You can rewire the kiln with all new elements that are rated for 208, add another element or just run with it. It's not going to harm your kiln running with less power.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:06 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.