coolant suppliers

I am looking for sources for diamond saw coolants. It seems that saw sales people don't usually handle the coolants. Any guidance would be most helpful. Most likely in one gallon bottles and not the CRL stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 09-12-2019, 01:37 AM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 442
David Hopman is on a distinguished road
I am using mineral oil from Tractor Supply Co. It is sold in gallon bottles as horse laxative. Ooh, new brand, cheaper at $14.99 a gallon. I use it in my 24" lapidary saw.

https://www.tractorsupply.com/tsc/pr...1&cm_vc=-10005
Reply With Quote
  #3  
Old 09-12-2019, 06:57 AM
Victor Chiarizia Victor Chiarizia is offline
Registered User
 
Join Date: Sep 2005
Location: fairview, NC
Posts: 579
Victor Chiarizia is on a distinguished road
i used to use coolmist blue stuff wont rust equipment and has oils for lube. cleaned up ez. vic
other stuff back in my scientific glass days came from lunzer industrial diamond in NJ don't remember anything else about it.
Reply With Quote
  #4  
Old 09-16-2019, 04:41 PM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
I too like the Mineral oil, Edcot is the brand name of ours. No rust, good for the blades and easy to recycle.
Reply With Quote
  #5  
Old 09-16-2019, 08:42 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Broken Clock
 
Join Date: Jan 2007
Location: Aarde
Posts: 2,221
Greg Vriethoff is on a distinguished road
Is the mineral oil used straight, or do you cut it with something else?
Reply With Quote
  #6  
Old 09-17-2019, 07:15 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,072
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Rollin Karg View Post
I too like the Mineral oil, Edcot is the brand name of ours. No rust, good for the blades and easy to recycle.
****
Well, what else is in the stuff besides mineral oil?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 09-23-2019, 09:52 PM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 442
David Hopman is on a distinguished road
Quote:
Originally Posted by Greg Vriethoff View Post
Is the mineral oil used straight, or do you cut it with something else?
Straight, no chaser.
Reply With Quote
  #8  
Old 09-24-2019, 06:30 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,072
Pete VanderLaan is on a distinguished road
Does that then make the workpiece far slippier to hold?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 09-25-2019, 02:50 AM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Does that then make the workpiece far slippier to hold?
There’s a sink next to the saw, easy to clean. You’ll have to clean it no matter what. We recycle both the oil in the saw and the water in the sink.
Reply With Quote
  #10  
Old 09-25-2019, 07:27 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,072
Pete VanderLaan is on a distinguished road
The felker sort of splashes stuff around. Most of the time I have a 14 inch blade on it, sometimes a 20 and sometimes a tiny 7 . Spray gets on the floor and this sounds sort of slippery. Rinse sinks are sort of an issue in this shop.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 09-25-2019, 05:40 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,704
Jordan Kube is on a distinguished road
When I worked as a glazier we used this stuff when drilling holes in glass:

https://www.amazon.com/CRL-Diamond-T.../dp/B00QL4JLHW

50:1 mix

It also comes in an 8 ounce bottle.
__________________
WWUD? Think for yourself.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:44 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.