Bullseye Furnaces and Baghouse

Does anyone know what type of furnace Bullseye uses? They appear to be to single pot gas fired. Any idea on what size?

And how does this baghouse work? I would assume all of the exhaust is going through but that would be high heat. The prototype they have shown appears to be a simple affair.
Reply With Quote
  #2  
Old 08-06-2017, 07:06 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,085
Pete VanderLaan is on a distinguished road
They can be bigger. It's essentially an enclosure that runs on positive suction and draws all the fumes ( door too) to a ceramic filter which must not be overheated. Gaffer uses an air conditioner to keep the filter cool. It gums up if it gets too hot. The filters are expensive . You can expect to spend $25-30K on the tooling for one. Here's a primary source:

http://www2.donaldson.com/torit/en-u...FVFbhgodRl0BUw
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 08-06-2017, 05:40 PM
Doug Terrell Doug Terrell is offline
Registered User
 
Join Date: Jan 2013
Location: Washington, IN
Posts: 15
Doug Terrell is on a distinguished road
It seems it would take quite a bit of energy to cool the flue gases. Or are the somehow keeping the glass fumes away from the burner/gas flue?
Reply With Quote
  #4  
Old 08-06-2017, 06:57 PM
Dennis Hetland Dennis Hetland is offline
Registered User
 
Join Date: Sep 2009
Location: Salem, OR
Posts: 304
Dennis Hetland is an unknown quantity at this point
Quote:
Originally Posted by Doug Terrell View Post
Does anyone know what type of furnace Bullseye uses? They appear to be to single pot gas fired. Any idea on what size?

And how does this baghouse work? I would assume all of the exhaust is going through but that would be high heat. The prototype they have shown appears to be a simple affair.
Someone that was a ladeler there told me they had a 2000lb crucible furnace

Does their bag house include a limestone slurry spray/bath?
__________________
candlewoodglass@gmail.com
Reply With Quote
  #5  
Old 08-07-2017, 07:36 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,085
Pete VanderLaan is on a distinguished road
1200 lb is my understanding but there are quite a few furnaces. .

The filter is not directly on the furnace. It's in the baghouse in line with the ventilation. If it gets too hot, the materials clog and stick to the filter which still has to be cleaned. Clogged ones are seriously clogged and don't survive but Donaldson will happily sell you another filter for large dollars .Gaffer put an AC unit on to keep the temps down at the filter. It's on a thermostat and is a very simple solution to the problem. It still needs a collection site which takes up space.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:28 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.