Polishing cast piece

So I have a larger, for me, cast piece Iím trying to finish. There are no flat surfaces so Iím doing everything with a right angle grinder. Itís working well and Iím down to 1500 but with diamond you can always see working lines on the surface.

Has anyone used loose grit by hand to grind something like this? I canít figure out what to use as a backer for the grit... if it was flat Iíd use another piece of flat glass. Could I use a sponge, rubber,???

Help
Reply With Quote
  #2  
Old 11-09-2017, 12:52 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Please Disperse
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 1,878
Greg Vriethoff is on a distinguished road
Hi Chris.

You can use a loose piece of felt, or even a green Scotchbrite pad.

I'm sure others will have more options, but these are the two things I am aware of.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #3  
Old 11-09-2017, 01:23 PM
David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 405
David Hopman is on a distinguished road
A piece of soft leather. There are also diamond pads- I use a 5000 grit one for hand sanding on sandblasted pieces.
Reply With Quote
  #4  
Old 11-09-2017, 01:25 PM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: New Jersey
Posts: 72
Marc Carmen is on a distinguished road
Ahhh welcome to one of the handful of coldworking processes that will actually drive you insane. Making it to a perfect cerium polish with no pitting or swirl marks is pretty tough to do with a hand grinder. You can come close to perfect very easily, but a perfect surface takes a lot of time and attention. I've seen Czech sculptures with very visible swirl marks.

I've tried everything. Electroplated diamond, SiC pads, resin smoothing pads, polpur, and resin pads for granite. They all kinda work for different things. Electroplated diamond scratches like hell and then wears out quick. SiC pads are alright. Resin smoothing pads (flat lap style) aren't very aggressive, clog and glaze over easily, and wear out quickly. Polpur snail lock discs work alright for stuff with a smaller point of contact (well curved surfaces). On flatter surfaces they hydroplane, and when you turn the water down they gall the surface and cause micro pitts. All these types of abrasive work so well on other machines and then just eat shit on a wet polisher.

The one thing I found that works Are the alpha ceramica pads. They're expensive as hell and theres a lot to learning how to use them. They have extremely soft resin compared to other stone polishing pads, so you're always exposing fresh diamonds. After I learned how to use them with a spongey backer, I got very consistent scratch marks right up to 1000 grit. Then I usually go felt and pumice, then felt and cerium. Sometimes I use a polpur 4" brown polishing wheel gorilla glued to a snail lock backer for a rough polish, then finish with felt and cerium.
Reply With Quote
  #5  
Old 11-09-2017, 01:42 PM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 206
Chris Lowry is on a distinguished road
Thanks guys... I think Iíll try the felt idea. This is my first piece and the casting isnít perfect so it is a nice one to experiment with.
Reply With Quote
  #6  
Old 11-09-2017, 02:47 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,576
Pete VanderLaan is on a distinguished road
You could also consider pumice on a piece of Rodel pad. Remarkably messy. Use a 0-3/4 pumice on a perforated pad. I use an air grinder with water feed. Wear a water proof suit and goggles. I just did a large piece of marble with it. Outside curves aren't bad. Inside curves are another matter.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 11-10-2017, 01:30 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 528
Charles Friedman is on a distinguished road
Try using Cratex bullet shape grinding and polishing Dermal bits.


https://www.riogrande.com/product/cr...ra-fine/332883
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #8  
Old 11-10-2017, 01:44 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,576
Pete VanderLaan is on a distinguished road
I've used cratex for tiny issues and in my clumsy hands, it just bounced too much as it was so small. In any polishing the issue is surface feet per minute and you need a fair amount to remove stock regardless of the grit size. Then the immediate problem becomes heat generation.

I think cerium on a felt is too fine for smoothing out those radial marks. I do think the pumice on rodel would work but again, be messy. I think you need at least a 3-4 inch diameter pad. Then you could go the cerium.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 11-10-2017, 02:20 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,547
Jordan Kube is on a distinguished road
We used to use one of these to polish scratches out of large mirrors. If you get one from CRL directly they are a little cheaper at $655.

https://www.dkhardware.com/heavy-dut...SABEgKPKPD_BwE

They also have cerium on sale right now for about $15/pound in 5 or 10 pound pails.
__________________
WWUD? Think for yourself.

Last edited by Jordan Kube; 11-10-2017 at 02:26 PM.
Reply With Quote
  #10  
Old 11-10-2017, 02:29 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,576
Pete VanderLaan is on a distinguished road
that looks to be a handy expensive thing Jordan.

I think you need to think about what polishing out a scratch really means. The scratch is deeper than anything around it so to get rid of it, you have to go that deep and that can be done crudely, and you'll see the removal as a shiny divot, or you can gradually lower the area around the scratch with sufficient skill as to not easily perceive the divot. Either way, one exists unless the issue stood proud of the piece.

Almost inevitably, a step in the removal goes too fast and the next step can't remove the last step. As Fenton said, "Glass remembers everything you ever do to it" and it could not be more true when you're trying to polish something with a curve in it.

That would be a nice price on the cerium if the cerium is any good and all ceriums are very different in quality. . Eveline brought me another 10KG bag of the Panda Brand when she was here in March. It's simply not sold outside of China. Nice little Panda chewing on Bamboo on the bag...
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 11-10-2017, 02:35 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,547
Jordan Kube is on a distinguished road
I remember one job where we installed a full wall in the dining room in this mansion on the cliffs over looking the ocean. One of the panels ended up with a deep scratch that the owner wanted out. We talked them through the process and explained the options. A light polish would make it look better but if we went too deep you would see it. They wanted it gone gone gone. One of the guys spent half the day leaning against the mirror with that machine to get it out. The owner ended up with a big fish eye where the scratch used to be. I thought it looked worse than the scratch but they seemed ok with it.
__________________
WWUD? Think for yourself.
Reply With Quote
  #12  
Old 11-10-2017, 05:08 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,576
Pete VanderLaan is on a distinguished road
Fenton's words are just totally immortal. RIP you old drunk.

"Glass remember's everything you ever do to it."

When you do anything, remember this one.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #13  
Old 11-13-2017, 07:14 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 790
Larry Cazes is on a distinguished road
3M makes diamond pads with sponge backing that are flexible enough to conform to rounded shapes and corners. I believe I got my last batch from HIS
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:19 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.