Looking for 106lb Pot

Hello everyone,

Anyone have a spare 106lb pot in the southeast they would sell me?

Mine got lost/delayed in the mail coming from Oregon and my rebuild is scheduled for next week....


Thanks,
Max
Reply With Quote
  #2  
Old 11-22-2017, 08:47 PM
phil taylor phil taylor is offline
Registered User
 
Join Date: Sep 2016
Location: cincinnati, ohio
Posts: 3
phil taylor is on a distinguished road
call up mobile glassblowing studios in americus,ga. they might have one. 229-352-9988
Reply With Quote
  #3  
Old 11-23-2017, 09:05 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 154
Max Epstein is on a distinguished road
Hey Phil, thanks for the advice!

UPS found my shipment and it'll be here Friday! Whhooooooohoooooo!
Reply With Quote
  #4  
Old 11-23-2017, 09:30 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
May be there Friday... UPS gets very interesting around holidays in terms of reasons for failures.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 11-24-2017, 10:54 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,086
Scott Novota is on a distinguished road
Strong Street had him covered up with one that was slightly smaller if it did not pop up for air from UPS.

We have 3 spares at this point that are 14.5. About to be two down in about 3 months as I fire up the color!

I swear Pete only teaches the color class to sell crucibles. It is my own personal glass conspiracy theory.
Reply With Quote
  #6  
Old 11-24-2017, 11:36 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Scott Novota View Post

I swear Pete only teaches the color class to sell crucibles. It is my own personal glass conspiracy theory.
***
Of course that's why I teach the class so regularly that people get utterly sick of it. When was the last one? 2012? You just think too small. I also have all those braided straps for molys. I'm no longer willing to sell cadmium or fluorine compounds. I still sell bad advice .
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 11-25-2017, 10:16 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 154
Max Epstein is on a distinguished road
Scott definitely had me covered!

Glad it showed up.... this thing is a work of beauty!

/cry
Reply With Quote
  #8  
Old 11-27-2017, 11:28 AM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,086
Scott Novota is on a distinguished road
Good lord has it been that long. 2012!

I am at less than one new color a year....
Reply With Quote
  #9  
Old 11-27-2017, 12:22 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,001
Pete VanderLaan is on a distinguished road
I'm pretty sure. We went to Shanghai in jan 2013, eveline came here for the class that June. Time flies when you're hurtling towards oblivion.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:51 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.