why didn't I think of that?

Im sure we have all seen someone do something with glass that makes you smack your head and say " Why didn't I think of that?". This one is for Pete..
Attached Images
File Type: jpg crucible art.jpg (18.7 KB, 154 views)
Reply With Quote
  #2  
Old 11-11-2017, 10:44 AM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: New Jersey
Posts: 76
Marc Carmen is on a distinguished road
OMG Eben I said the same thing when I saw that. It really is a great idea. Especially aesthetically pleasing for glassmakers.
Reply With Quote
  #3  
Old 11-11-2017, 03:40 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,617
Jordan Kube is on a distinguished road
Super cool. I have a billion of those crucibles lying around. Maybe a fun new project!
__________________
WWUD? Think for yourself.
Reply With Quote
  #4  
Old 11-14-2017, 05:32 PM
Scott Novota's Avatar
Scott Novota Scott Novota is offline
AbbyNormal User
 
Join Date: Jan 2004
Location: Pensacola Florida
Posts: 2,098
Scott Novota is on a distinguished road
I have one of these in the shop but the color inside is scrap Pete sent me from a silver opal melt from about 8 years ago. It has spider webbing around the crucible but looks a lot like this. Home depot tile saw and 10 min on the lap.

Mine was not a controlled anneal....Not near as good looking. I use to to show people what is going on inside the furnace when I have open houses.
Reply With Quote
  #5  
Old 11-14-2017, 07:12 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,306
Eben Horton is on a distinguished road
No comment from Pete yet. He must be digging through his cullet pile ! Hehehe
Reply With Quote
  #6  
Old 11-16-2017, 07:48 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,266
Pete VanderLaan is on a distinguished road
Oh I like it, believe me. I don't have cullet piles but I do have 50 bags of most everything.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 11-16-2017, 09:48 AM
Jeffrey Mentuck Jeffrey Mentuck is offline
Registered User
 
Join Date: Mar 2016
Location: Salem
Posts: 13
Jeffrey Mentuck is on a distinguished road
Credit where it's due, Who is the Artist?
Reply With Quote
  #8  
Old 11-16-2017, 09:58 AM
John Riepma John Riepma is offline
Registered User
 
Join Date: Apr 2003
Location: Grand Haven, MI
Posts: 477
John Riepma is on a distinguished road
That's Anna Riley. I spoke with her for a while at Corning last year where she was an Artist in Residence doing some studies on decolorizing glass, and she showed me some of the crucibles that she had used for prior melts. They looked just like that.
Reply With Quote
  #9  
Old 11-16-2017, 11:27 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,358
Rich Samuel is on a distinguished road
These will make you cry.

http://www.wheatonarts.org/anna-riley/
Reply With Quote
  #10  
Old 11-16-2017, 01:52 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,617
Jordan Kube is on a distinguished road
Well the one with 35% sodium sure melted down better!
__________________
WWUD? Think for yourself.
Reply With Quote
  #11  
Old 11-16-2017, 02:46 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,266
Pete VanderLaan is on a distinguished road
I was looking at those numbers too.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:30 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.