Sky Campbell is on a distinguished road
There is no convection in an electric furnace

It's been a little slow and I thought some may find this interesting.

Movement of heat through convection ends at around 1100 degrees F. At 1700 F, a cubic foot of air has only about one-tenth the number of molecules as at room temperature. This is why there is little airflow at high temperatures.
Reply With Quote
  #2  
Old 09-05-2017, 03:50 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 613
Lawrence Duckworth is on a distinguished road
We had to call a serviceman to come out and try to fix my wife's convection cooktop in our new "forever home" ....He couldn't fix it, just simply didn't know what was wrong with it. Turns out ya gotta use stainless steel cookware
...I came close to buying a convection forge awhile back, would have been just the thing for spider legs!
Reply With Quote
  #3  
Old 09-05-2017, 06:33 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is online now
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 857
Sky Campbell is on a distinguished road
Induction heating probably deserves its own thread but I'll tell you first hand induction forges are well worth the money. I'm blown away at the speed and the ability to localize heat. You can buy one of the import induction forges for way less then you would imagine. I'd also guess you have a water cooler from your tig. Anyway Bill Roberts bought one just for fireplace tools you should ask him about it.


I also bought into the induction cooktop craze and if I knew it was going to be so noisy I would have stayed with gas. As a matter of fact ours was so loud we yanked it and it now lives in the shop. Yours is probably of better quality with quieter cooling fans.


Anyway splurge a little Duck buy an induction furnace it's really perfect for some of your work. I know you'll love it.


Now how can we apply it to glass. I wonder if sic heats with induction. I'll try it and let you know in a bit.
Reply With Quote
  #4  
Old 09-05-2017, 07:10 PM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 613
Lawrence Duckworth is on a distinguished road
her's is a Kitchenaid Convection Cooktop, doesn't make any noise at all but works only if you use stainless steel cookware, go fig'r.

I really would like to have an induction forge. It's fun to say induction out loud too.
Reply With Quote
  #5  
Old 09-05-2017, 08:40 PM
Brian Wong Shui Brian Wong Shui is offline
Registered User
 
Join Date: Oct 2002
Location: Atlanta, GA
Posts: 155
Brian Wong Shui is on a distinguished road
Magnetic. Anything attracted to a magnet will work. Can be clad. So....certain stainless steels will not work on the cooktop. Big heavy lodge cast iron will work perfectly 😀. Copper will not work.

It's amazing how fast an induction cooktop will boil a pot of water for pasta.
Reply With Quote
  #6  
Old 09-06-2017, 12:42 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 463
Art Freas is on a distinguished road
Was watching a show where they melted gold in a table top induction unit. Amazing how fast it melted the gold just sitting on a table top.
Reply With Quote
  #7  
Old 09-06-2017, 12:47 AM
David Hopman David Hopman is online now
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 417
David Hopman is on a distinguished road
Is anybody here using an induction coil as a pipe warmer?
Reply With Quote
  #8  
Old 09-06-2017, 07:00 AM
Lawrence Duckworth Lawrence Duckworth is offline
Registered User
 
Join Date: Mar 2010
Location: Gainesville, GA
Posts: 613
Lawrence Duckworth is on a distinguished road
Quote:
Originally Posted by Sky Campbell View Post
It's been a little slow and I thought some may find this interesting.

Movement of heat through convection ends at around 1100 degrees F. At 1700 F, a cubic foot of air has only about one-tenth the number of molecules as at room temperature. This is why there is little airflow at high temperatures.

Ok Sky, I see how I confused things. A convection oven cooks more evenly because a fan circulates the hot air, and if I read you that has some limits of around 1100f?

donno how I got caught up in the "Induction" thing

btw, hope Irma makes a U turn!!
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:45 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.