No, No,... batch encapsulated in Hxtal. Double your toxins.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #77  
Old 05-03-2019, 08:44 AM
Pringle Teetor's Avatar
Pringle Teetor Pringle Teetor is offline
Registered User
 
Join Date: Jul 2003
Location: Chapel Hill, NC
Posts: 658
Pringle Teetor is on a distinguished road
You do need a good sense of humor and a tough shell to be a participant of this board sometimes. When I first came on I was scared to post for a while, the. Got the gist of it - lots of fun poked but more importantly - good information and lots of opinions. Now if only someone could tell me a trick about seeing what I need to see when I solo punty, now that I’m over 60. No depth perception...... someone would probably say “ best solution? An assistant”.
Reply With Quote
  #78  
Old 05-03-2019, 08:51 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 585
Shawn Everette is on a distinguished road
Well, yes, an assistant is best, but they come with their own issues. Have you tried marking with chalk or a shard?
Reply With Quote
  #79  
Old 05-03-2019, 09:23 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,933
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Well, yes, an assistant is best, but they come with their own issues.
*****
Understatement of the year.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #80  
Old 05-03-2019, 04:37 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is online now
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,170
Richard Huntrods is on a distinguished road
Quote:
Originally Posted by Pringle Teetor View Post
You do need a good sense of humor and a tough shell to be a participant of this board sometimes. When I first came on I was scared to post for a while, the. Got the gist of it - lots of fun poked but more importantly - good information and lots of opinions. Now if only someone could tell me a trick about seeing what I need to see when I solo punty, now that I’m over 60. No depth perception...... someone would probably say “ best solution? An assistant”.
I use a pair of box store 500W halogen 'work lights'. The ones that come on a stand are best as you can move them around to find the best placement. I have them angled differently so the combined light blast gives me some real 'depth of field' (i.e. dramatic shadows) as I get close to 'touchdown'.
Reply With Quote
  #81  
Old 05-05-2019, 01:07 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Triggered
 
Join Date: Jan 2007
Location: Aarde
Posts: 2,218
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Survives Nuclear Holocausts...
Where would you get real-world testing for this claim?
Reply With Quote
  #82  
Old 05-05-2019, 01:15 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,933
Pete VanderLaan is on a distinguished road
Just ask your national government to distract the voters for a few hours. Place the sample in a likely location... Korea... Venezuela.. Sudan..Iran

Bask in the reassuring glow.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #83  
Old 05-16-2019, 08:54 AM
Laura Doerger-Roberts's Avatar
Laura Doerger-Roberts Laura Doerger-Roberts is offline
Registered User
 
Join Date: Apr 2004
Location: Cincinnati, OH
Posts: 519
Laura Doerger-Roberts is on a distinguished road
Well, I have been guilty of lurking on and off for years, occasionally posting, and finding it best to just stay in my lane, which is that of a hobbyist with limited tech and chemistry experience.

This board has not changed as much as other technology for sharing information has. The scant other women glassblowers I know seem to be mostly younger than my 49 years, and if I generalize, they are more interested in technique for creation of their art, rather than the nuts and bolts of furnaces, glass chemistry, COE, fit, equipment building, running a shop, batch composition. And, if it can be illustrated with a photo or video, all the better.

I regularly ask people if they are on here or have seen a post on here and I get a lot of blank stares. Too bad for them. I consider the regulars here to be a council of my elders who have vastly more experience and knowledge than I do. The archives are a masterpiece. I read the board regularly, absorb what I can, but more importantly know what kind of questions are best to ask here and love the earnest responses that generally come through.

I'm not uninterested in the mechanics and the science, but as a hobbyist, I don't have my own shop, and have limited amounts of time to pursue glass. I don't bother to pester this board about opinions on color combinations, or techniques with powders, or how to create the art. To me, that's the essence of creating art that is uniquely mine. Figure out how to create it. Most of my glass-related wonderings are on those types of topics. But, when I have a technical question, I come here.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:51 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.