My heating coil need to cross over or under the thermocouple.
I am thinking about stretching the coil and slipping it under or over the thermocouple. Any warning or comments?
Franklin
Reply With Quote
  #2  
Old 06-15-2019, 03:37 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,953
Franklin Sankar is on a distinguished road
This is a drawing of what I want to do. Hope it donít rotate.
Franklin
Attached Images
File Type: jpg F32F400C-B8B8-4198-BD04-8B08F92FFBBE.jpg (20.2 KB, 23 views)
Reply With Quote
  #3  
Old 06-15-2019, 07:02 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 976
Sky Campbell is on a distinguished road
I would drill a new hole for the thermocouple before I would do anything to change the element. Every little thing you do like that causes uneven heating and stress to the element. Maybe just drill and angle the thermocouple above the element.
Reply With Quote
  #4  
Old 06-15-2019, 07:02 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,566
Pete VanderLaan is on a distinguished road
further away would be better.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 06-15-2019, 08:44 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,953
Franklin Sankar is on a distinguished road
Thanks . Wise hints well noted

Franklin
Reply With Quote
  #6  
Old 06-16-2019, 09:15 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,953
Franklin Sankar is on a distinguished road
Sky you mentioned something very important about the groves for the coils but I canít find it now. It was something about the shape of the grove and the reflected heat in the grove.
Can you remember?
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:00 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.