Can I mix color rod with clear cullet?

I have an order for a lot of opaque black glass. I work from an electric wound-wire element furnace which maxes out around working temp and won't melt batch. I am melting Bomma cullet, in a 55 pound capacity crucible and it works for me.

I bought 15 kilos of Reichenbach black, but it's somewhat slow and wasteful to use a piece of the color bar for each blown piece I make, as the finished pieces are about the size of a grapefruit.

I have an old crucible at the end of it's productive life. It occurred to me that I may be able to melt the black rod into clear glass in that crucible and just make all my black pieces from the furnace.

The method that occurs to me is to cut the rod up into slices, and then 1/4 slices and put in about 6 nuggets of the Bomma cullet with each 1/4 slice of black rod. Total of about 8 pounds per charge, let it melt to liquid state, and stir with a punty like twice for 15 seconds each time.

It sounds really sloppy and like I will probably get strands of black and strands of clear in the final piece. Even if I returned the rod and used frit, I don't have much faith it will yield a smooth black glass body.

Any thoughts on a way to use the color rod and clear cullet? Or should I just order black cullet from Gabbert?

Thanks for any input!
Brice
Reply With Quote
  #2  
Old 03-18-2022, 02:58 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
Likelyhood of this working is about "0". The color rod is likely a 24% lead and your cullet is a soda lime. Melted together they will resemble oil and water. Cordy, really cordy.. The rod wants to be melted very cold to retain it's color. Once Dale made me do this with Tabac and it turned to absolute shit at about 2100F 1800 might have worked better but still, not a good plan.

I think you'd be better off adding cobalt, manganese, nickel and Pot dichromate at about .01% to the Bomma. Go from there. It will likely need some soda ash to bring the expansion into line.
To get this into perspective, my dense black has 19 pounds of colorants in every 100 lbs of glass and the glass is a lead base 10%. It certainly is black. Frit will look like frit on clear.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-18-2022, 10:50 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 1,433
Michael Ahlefeldt-Laurvig is on a distinguished road
Why is it wasteful for you to use the color bar on your pipe? Real dense black (at least) used to be difficult to find as rods
How many pieces?

Last edited by Michael Ahlefeldt-Laurvig; 03-19-2022 at 05:31 AM. Reason: Last question
Reply With Quote
  #4  
Old 03-19-2022, 09:41 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
well, it's time consuming and takes an assistant that one presumes gets paid.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-19-2022, 09:22 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 1,433
Michael Ahlefeldt-Laurvig is on a distinguished road
If you dont have an assistant, who will you blame when things F up?
Reply With Quote
  #6  
Old 03-20-2022, 12:28 AM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,944
David Patchen is on a distinguished road
Quote:
Originally Posted by Brice Turnbull View Post
I bought 15 kilos of Reichenbach black, but it's somewhat slow and wasteful to use a piece of the color bar for each blown piece I make, as the finished pieces are about the size of a grapefruit.
Stick up half a rod at a time and overlay only enough for what you need. It should take your assistant about as long to heat the end of the color rod for an overlay as it will for you to make a starter bubble. The assistant garages the rest of the rod after you take the overlay. Superfast. Alternatively you could also make lots of supios out of a long tube of black and saw them up cold then heat them in the garage, but that still seems slower.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:47 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2023, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.