grey tinted glass from color scrap

I saved up a few hundred lbs of scrap glass, moils, trimmings etc. Melting a pot of this stuff of course yields that nice blue tinted glass. Adding 10% batch to this and stirring while melting makes the color consistent and bubble free. Now, I’d like to try shifting this pale blue towards a neutral grey while still maintaining a light tint. Does anyone have any experience or input they can share?

I suspect using a pinch of nickel would just make a green/grey the way it does in combination with cobalt.

Maybe the right manganese/chrome combo could oppose the blue nicely but manganese is so unreliable in low concentrations.

Selenium or Iron/selenium? I don’t have much experience with selenium but as I understand it, Iron and selenium make a red/brown? What percentage of selenium do I add before it begins to show color? My glass is sodium based.
Reply With Quote
  #2  
Old 12-22-2021, 08:18 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,091
Pete VanderLaan is on a distinguished road
manganese and iron.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 12-22-2021, 10:20 AM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 923
Josh Bernbaum is on a distinguished road
I'd guess selenium will steer you more towards brown if you're base is mostly sodium for your alkali. Manganese and iron added to SP (all sodium) gets me a light amber or tea type result which I've preferred to having to do a typical amber and then have to deal with the sulphur odor. But maybe if you have the blue tint already, then adding those two will have it go more light grey for you with Pete's recommendation. There seem to be lots of ways to get to a grey when looking through the old factory formulas. One of the things John and I had emailed about was minute changes in proportions of nickel, cobalt, and copper for getting a light grey shade that's to your liking. I did get to a light grey I really liked, but there was at least some potassium in that mix for whatever that is worth.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 12-22-2021, 11:01 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,091
Pete VanderLaan is on a distinguished road
I was assuming the base cullet was already a washed out blue. You can only add so much crap to cullet before it goes cordy on you.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 12-23-2021, 10:44 AM
Ed Pennebaker's Avatar
Ed Pennebaker Ed Pennebaker is offline
Registered User
 
Join Date: Apr 2002
Location: Red Fern Glass in Clinton, Arkansas
Posts: 235
Ed Pennebaker is on a distinguished road
I've made grays from Spruce Pine 87 plain several times. 100 pounds of batch. .25 gm cobalt oxide to 8 gm nickel carbonate was greenish gray
.5 gm cobalt to 8 gm nickel was good
1 gm cobalt to 8 gm nickel was bluish gray
It is pretty touchy. I was also using some cullet from previous batches in each batch. It is pretty light gray. I was using it to blow single color transparent pieces.
__________________
Make, fix and create. Assist others in learning lifewise. (From Doug Stowe's blog Wisdom of the Hands)
Reply With Quote
  #6  
Old 12-23-2021, 10:54 AM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: Rahway, New Jersey
Posts: 105
Marc Carmen is on a distinguished road
Ohhh yeaaa, manganese and iron. Thanks, I’ll try that today.

Yesterday I tried a small addition of manganese/chrome. The ratio was one that would normally make a reddish brown in higher concentrations. It did turn the glass greyer, but also greener. I guess I could just keep adding manganese.

Josh, I’m interested in the grey from cobalt, nickel, and copper because those are pretty reliable colorants. For me, any combination of nickel and cobalt will get the whole range of smokey blue-greens but never quite go neutral grey. It doesn’t seem like copper could help. Maybe the potassium in your batch is shifting the nickel towards a warmer tone. I always had to add manganese/chrome in my grey color bar melts.

Cords never seem to be a problem. All the crap cullet was quenched in water and turned into relatively fine frit and small chunks. I also stir the melt with a punty in a drill with a cold gather on the end.
Reply With Quote
  #7  
Old 12-23-2021, 12:31 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,091
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Marc Carmen View Post
Ohhh yeaaa, manganese and iron. Thanks, I’ll try that today.

Yesterday I tried a small addition of manganese/chrome. The ratio was one that would normally make a reddish brown in higher concentrations. It did turn the glass greyer, but also greener. I guess I could just keep adding manganese.

Josh, I’m interested in the grey from cobalt, nickel, and copper because those are pretty reliable colorants. For me, any combination of nickel and cobalt will get the whole range of smokey blue-greens but never quite go neutral grey. It doesn’t seem like copper could help. Maybe the potassium in your batch is shifting the nickel towards a warmer tone. I always had to add manganese/chrome in my grey color bar melts.

Cords never seem to be a problem. All the crap cullet was quenched in water and turned into relatively fine frit and small chunks. I also stir the melt with a punty in a drill with a cold gather on the end.
****
Try the potato. It mixes really well.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 12-26-2021, 02:54 PM
Marc Carmen Marc Carmen is offline
Registered User
 
Join Date: Jul 2015
Location: Rahway, New Jersey
Posts: 105
Marc Carmen is on a distinguished road
Planning on trying the potato soon since I recently moved up from a wire melter to a gas furnace.

Manganese and Iron looked very promising while melting in. A nice neutral grey. After fining that changed back to a dull blue. I guess it's the same deal as manganese/chrome, I could just keep adding manganese til it greys out the blue.

What ended up working was adding tiny bit of nickel for a green grey and then neutralizing the green cast with erbium. Very stable color and its not a prohibitively expensive amount of erbium either.
Reply With Quote
  #9  
Old 12-26-2021, 04:03 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,091
Pete VanderLaan is on a distinguished road
Any reduction in the flame burns out manganese if it is actually gas.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:25 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2023, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.