CraftWEB Hot Glass Talk  

Go Back   CraftWEB Hot Glass Talk > Color work from rods and batch glasses

Reply
 
Thread Tools Display Modes
  #1  
Old 03-28-2022, 09:27 AM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 921
Josh Bernbaum is on a distinguished road
Red Peachblow?

I ran across a couple images recently of some old work made by the LE Smith factory. I'm not attaching them here because they seem to be super small files and I think it'll come across pretty pixelated, but the look of these vases reminded me of what I've seen of Peachblow but less 'peachy' and more of a bright red. Would this still be considered a type of Peachblow, I suppose with more cadmium to go with the selenium? They look to me like what I imagine the straw-to-bright red strike on a transparent cad/sel fade would look like but in opaque form. But I'm not used to seeing 'heat-history' striking with opaque reds as with the transparents.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #2  
Old 03-28-2022, 10:34 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
I think you probably still have the formula we used for a fluorine opal peach back in the classes. It is a thermal glass if you want to strike it. By puntying the stuff and reheating it just at the lip, it strikes that way. Differing base glasses would yield differing results. Casing it changes things and not necessarily in a good way.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-28-2022, 11:16 AM
Terry Crider Terry Crider is offline
Registered User
 
Join Date: Jan 2020
Location: Ohio
Posts: 7
Terry Crider is on a distinguished road
Without a pic - I'm not sure what you are asking; but google "Plated Amberina"
Is it anything like this?
Reply With Quote
  #4  
Old 03-28-2022, 12:03 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
That's the stuff. You can see where it was put in a ribbing mold which chilled part of the piece and it darkened at those points. As you drop down the piece, the ribbing did not go with it. If the mix was kept cold, it never struck. If heated after that chilling, it strikes great.

Very popular in the great depression period since it was a lot of flash for not much cash. Basically a fluorine with cadmium sulfide and selenium in it. Probably harder to do then I make it sound. I used to do it on stemware when the cup was blown out and a stem attached, then a foot. The reheat involved just getting the lip pretty hot, trimming it and opening. These pictures look better than mine was although I never worked at perfecting it. I liked what I had.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-28-2022, 12:18 PM
Terry Crider Terry Crider is offline
Registered User
 
Join Date: Jan 2020
Location: Ohio
Posts: 7
Terry Crider is on a distinguished road
Pete,
I don't know anything the Lead/Arsenic White that you have talked about from time to time; but the interior White casing on any of this is very very thin and still very opaque.
Is that what the casing on this is?
Reply With Quote
  #6  
Old 03-28-2022, 12:37 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
I don't know. My fluorine white can be very thin and very opaque . My stuff was a fluorine that had selenium and cadmium in it but it's hard to get right. It was not brilliant in the red struck part The portion of the spectrum for red is incredibly small so slippage tends to make it either orangey or brown. Keeping white out of the mix makes for a better color in my opinion.

When Gaffer was first going, John made a gorgeous Ferrari red but the color slipped its moorings eventually. It worked as a lip wrap.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 03-28-2022, 07:04 PM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 921
Josh Bernbaum is on a distinguished road
Quote:
Originally Posted by Terry Crider View Post
Without a pic - I'm not sure what you are asking; but google "Plated Amberina"
Is it anything like this?
Well most of that search showed more of what looked like a gold ruby fade over a fluorine white to me. But in another search I did see the word Amberina used to describe a similar LE Smith produced vase like I was talking about, which had a really nice opaque red as part of the strike and fading out to that opaque 'straw' color at the bottom. Pete, I remember that original Ferrari of John's, it was such a nice red.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #8  
Old 03-31-2022, 08:52 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 5,101
Eben Horton is on a distinguished road
Gaffers Ferrari morphed into vermillion and then into carmine which them crescendo’d into “original carmine” which was double the price.


Josh, if you know david Mcdermitt, ask him for a peach blow recipe. He has all of sandwich glass and pierpoint’s color recipes
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #9  
Old 03-31-2022, 09:26 AM
Josh Bernbaum Josh Bernbaum is online now
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 921
Josh Bernbaum is on a distinguished road
I don't know him, but I could look into contacting him. So is he a "sharing" kind of guy?
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #10  
Old 03-31-2022, 09:59 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
The mine runs coupled up with furnace and burner locations actually do make a huge difference not to mention altitude. Lino used to say "Melt glass where it wants to be melted" . The Germans said " A good recipe can't cross the street."

Croucher added, "Or the studio."

And they're all right. But I don't believe for a second that it has gold in it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 03-31-2022, 07:05 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 24,079
Pete VanderLaan is on a distinguished road
The real concern over lithium is whether it will raise the price of SP87 which is already ridiculously inexpensive compared to anything else out there.

You really don't need lithium in a batch glass. Substituting either calcium fluoride or potassium salts would suffice
making it melt colder. as long as you aren't running electric. If you use cullet, it does not matter at all.

In my black, I do bathe the potassium dichromate in a crushed compilation to get it to melt a bit easier. I could change that.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:35 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2023, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.