Dark Bottle Green Recipe

Hi there! It's been an awfully long time since I was here, but thought I would ask a question. I hope everyone is doing well!

Does anyone have any recommendations for a dark bottle green recipe? We melt Gaffer Batch here at the Canberra Glassworks. I have a recipe for a tealy-green but it is not dark enough.

Per batch of 100kg it is:

Iron 500g
Cobalt 1g
Nic 1g
Copper 20g

I saw this thread from 2014:
http://talk.craftweb.com/showthread....n+glass+recipe

I have attached an image of the density we're after as inspiration. I have also attached some pics of samples of teal greens that we already melt, they're too light. Any suggestions? How about this one below?

Olive Green Bottle Glass
sand 100 kilos
potassium chromate 500 grams
manganese dioxide 1500 grams

If anyone has any recommendations that would be wonderful.
Thank you!
Attached Images
File Type: jpg Dark Green inspiration.jpg (43.2 KB, 54 views)
File Type: jpg Light Teal Green.jpg (22.7 KB, 45 views)
File Type: jpg Light Lagoon Green.jpg (24.0 KB, 44 views)
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:23 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.