Opaque cullet

I don't remember this as an option but is it possible to make opaque glasses from cullet?

Really great stuff Dave, thanks for posting all that archived knowledge.
__________________
WWUD? Think for yourself.
Reply With Quote
  #2  
Old 12-22-2016, 02:38 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,666
Pete VanderLaan is on a distinguished road
The boro guys have been doing it adding zirconium to the pyrex cullet, or so I've heard. I can't see it doing anything that you would want to make for Mom at Christmas out of a soda Lime though. The Silver and copper colloidals are the closest thing I can imagine in that vein.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 12-22-2016, 02:47 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,666
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Jordan Kube View Post
I don't remember this as an option but is it possible to make opaque glasses from cullet?

Really great stuff Dave, thanks for posting all that archived knowledge.
*******
The big concern I have with it being posted without attribution is copywrite. Way back when, We had a guy named Mike Firth who was essentially lifting anything he found on the internet and asserting that it was public domain given the source. We had a glassworker named Graham Stone in Australia who had published his major works, "the schedules" which is an essential book to have if you want to do big castings. Firth essentially lifted stuff that was mine word for word, paragraph after paragraph as well and asserted his right to do it and publish it on his website with no permission to do so. The net effect was to sufficiently scare Graham to where he withdrew entirely from the Glass community. Everything on Craftweb is in fact copywrite protected but it gets a lot harder when you don't have the essential attribution of source. Everything Dave dug out had original source. I think having it out there is for the most part, great stuff but I really want to see the source authorship. I recognize a good deal of it is mine but it isn't all mine.
In my last and final color class I had a student simply start to make the formulas as color rods and really undercut my price. I essentially told him he was in copyright violation so he switched methodology. It really does actually hurt. Sharing is important. So is integrity.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 12-22-2016, 11:54 PM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,949
Dave Bross is on a distinguished road
I can go back through my original posts and tag the names onto the info to the best of my memory.

Most of what I posted is either Pete or me anyway.


Pete,

You're welcome to go through my posts and tag what's yours too.

If there's a link in the post is that enough or do you want the name on there too?
__________________
Art is not a thing...it's a way.
Reply With Quote
  #5  
Old 12-23-2016, 12:03 AM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,949
Dave Bross is on a distinguished road
Jordan,

Opaque from cullet is probably not easily do-able.

Too much calcium in cullet to go with phosphates and I seem to remember the experiments in Washington state trying for viable commercial colored glasses from bottle cullet couldn't get a fluorine opaque to work.

I'll see (or anyone else?) if I can find where all that Washington state info is online. I'm sure it's still out there somewhere and it would be a good addition to this section.
__________________
Art is not a thing...it's a way.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:15 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.