Centrifuge molds

We recently acquired a second hand Essemce centrifuge machine and just wondered if anyone (mainly European based as we are in the UK) knows of a mold maker with experience with these...or someone that has pre-existing molds that they might part with?

Many thanks for any help in advance...
__________________
www.rothschildbickers.com
Reply With Quote
  #2  
Old 12-19-2019, 01:33 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,441
Tom Fuhrman is on a distinguished road
When I was at Reidel in Austria many years ago, they were doing some centrifuge casting. You might check with them .
Reply With Quote
  #3  
Old 12-20-2019, 11:19 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 768
Michael Ahlefeldt-Laurvig is on a distinguished road
http://www.formverkstad.se/
Thomas makes almost everything for the swedish glass industri
Reply With Quote
  #4  
Old 12-21-2019, 02:36 AM
Mark Bickers Mark Bickers is offline
Registered User
 
Join Date: Oct 2010
Location: London, UK
Posts: 65
Mark Bickers is on a distinguished road
Tom - Thanks for tip, I will drop them a line and see where I get to.

Michael - I sent over an email and unfortunately was told that Thomas has retired. However they helpfully passed me on to another mould maker also based in Sweden. Be interesting to see where it goes.
__________________
www.rothschildbickers.com
Reply With Quote
  #5  
Old 12-21-2019, 08:46 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 768
Michael Ahlefeldt-Laurvig is on a distinguished road
Would that be Gunnar Englund? Hes a really nice guy and a great sculptur in his own right.
Gunnar makes mostly wood molds, or at least used to.
Thomas made lots of graphite molds, cnc milling, turnning on a lathe.I wonder whos taken over
Reply With Quote
  #6  
Old 12-22-2019, 02:46 AM
Mark Bickers Mark Bickers is offline
Registered User
 
Join Date: Oct 2010
Location: London, UK
Posts: 65
Mark Bickers is on a distinguished road
Michael - it was Håkan Karlsson from Mejk Verktyg AB. Now I just need to work out how to wrestle a SketchUp model into a IGES file format!
__________________
www.rothschildbickers.com
Reply With Quote
  #7  
Old 12-22-2019, 09:42 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,616
Eben Horton is on a distinguished road
If you know what you want and can source a big chunk of graphite, any machinist with a CNC router can cut you a mold. Just warn them about graphite dust and tell them to stick a shop vac hose next to the cutting head.
__________________
<eben epoiese>
Reply With Quote
  #8  
Old 12-22-2019, 12:06 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,441
Tom Fuhrman is on a distinguished road
Eben, are you sure that graphite is the best material for centrifuge casting? I would think it would be steel or iron as they may take a lot more abuse.
Reply With Quote
  #9  
Old 12-22-2019, 01:13 PM
Terry Crider
Guest
 
Posts: n/a
I watched Mosser Glass in Cambridge,Ohio spin out some (what to me was giant sushi platters).
They was dumping what looked like 6/7 pounds of glass in the center and spun out to about 3 ft. dia.
The way the glass flowed across the mold - I don't think graphite would last long and probably end up with contamination on the bottom.
They would probably send you to Island Mould --- your wallet would probably be a whole lot lighter, but anything you got from them would last a couple of life times.
Terry
Reply With Quote
  #10  
Old 12-22-2019, 05:20 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 768
Michael Ahlefeldt-Laurvig is on a distinguished road
On essemce web site go to contact and write and ask Jan Melin who makes metal molds now. Jan will know
Reply With Quote
  #11  
Old 12-22-2019, 07:48 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,616
Eben Horton is on a distinguished road
Quote:
Originally Posted by Tom Fuhrman View Post
Eben, are you sure that graphite is the best material for centrifuge casting? I would think it would be steel or iron as they may take a lot more abuse.
Well, sure. But is he going to make millions of pieces?
__________________
<eben epoiese>
Reply With Quote
  #12  
Old 12-22-2019, 08:42 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,441
Tom Fuhrman is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Well, sure. But is he going to make millions of pieces?
Like terry Crider said m when you're slinging several pounds of hot glass into a mold the chances of graphite deteriorating or busting can be very high. If he could make the right contacts there are some Indian companies that can do the molds fairly reasonable. A lot of it depends on the size and the detail required in the mold. Graphite might also be a problem because it will not suck enough heat out of the glass quick enough which is required in casting or pressing. It has to put a cool skin on the glass quite quickly as most centrifuge casting pieces are fairly thick.
Reply With Quote
  #13  
Old 12-23-2019, 07:59 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,714
Pete VanderLaan is on a distinguished road
Poured glass into graphite makes it pretty porous pretty fast, even high density ones.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:18 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.