"Adjusting" shear blades

I got a new pair of Maruko diamond shears as a thanks for a couple cherry wood blocks I made for a friend with the rather ambiguous caveat that said shears need to be "customized to cut right". And they don't (I'm spoiled after using Carlo Dona shears). The blades don't meet right and significant sideways force is needed to get them to meet and cut right.

My question: Is there a "proper" or better way to bend or cold forge shear blades so they meet and thus cut right? They are thin. What should be the focal point? Hammer? Mallet? Bench Vice? Don't even try?

Thanks for any advice
Reply With Quote
  #2  
Old 10-31-2017, 12:57 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,504
Rich Samuel is on a distinguished road
Did you possibly get a prototype? ( https://www.reddit.com/r/glassblowin..._cutting_edge/ )
Reply With Quote
  #3  
Old 10-31-2017, 07:32 PM
Travis Frink Travis Frink is offline
Registered User
 
Join Date: Feb 2008
Location: Tokushima, Japan
Posts: 617
Travis Frink is on a distinguished road
Could be. I don't know. Sounds like the same problem I'm having. I'd just like to get them to cut better. They are the coolest looking diamond shears I have but I'm not much for using tools as decorations.
Reply With Quote
  #4  
Old 10-31-2017, 08:50 PM
Scott Dunahee's Avatar
Scott Dunahee Scott Dunahee is offline
Registered User
 
Join Date: Apr 2002
Location: Madison, WI
Posts: 638
Scott Dunahee is on a distinguished road
I have sent tools to Jim Moore to be tuned up before. He did a remarkable job with some old esemce (sp?) shears I had.

Just an idea.

BSD
__________________
That's all right. I never expected there to be a blue light special on enlightenment...
Reply With Quote
  #5  
Old 10-31-2017, 10:06 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,603
Eben Horton is on a distinguished road
Take them apart.. one side has threads for the bolt that holds them together, and the other side doesn't have threads. take an open end socket and tighten that bolt so that the shears feel tight, but not too tight. Then without moving the bolt, thread on the nut and with one hand on the wrench that is holding the bolt, take another wrench and crank down on the nut so that the nut compresses against the side of the shear. if you move that bolt at all, you will throw off the tuning you just did.
Reply With Quote
  #6  
Old 10-31-2017, 11:39 PM
Travis Frink Travis Frink is offline
Registered User
 
Join Date: Feb 2008
Location: Tokushima, Japan
Posts: 617
Travis Frink is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
Take them apart...
I tried that. The blades don't meet without significant sideways pressure while cutting. The blades look like they need to be bent slightly to meet properly.

If Jim Moore was closer, I might ask him. Then again I kind of like the idea of learning and then being able to maintain my of tools.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 07:08 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.