  #1  
Old 03-14-2021, 03:34 PM
David Hopman David Hopman is online now
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 447
David Hopman is on a distinguished road
physicists on mystery-why does glass exist?

https://www.wired.com/story/physicis...uN1p7y3UQ8P77o
Reply With Quote
  #2  
Old 03-16-2021, 10:42 AM
Paul Thompson Paul Thompson is offline
Registered User
 
Join Date: Apr 2007
Location: Silver Spring MD
Posts: 205
Paul Thompson is on a distinguished road
Quote:
Glass is a liquid in suspended animation, a liquid whose molecules curiously cannot flow.
I thought the "glass is a supercooled liquid" theory had been largely discarded? And I don't think the process of plant amber hardening is the same as melted glass cooling. It seems like amber would harden via sublimation or evaporation.
__________________
"You don't have to be a very good glassblower when you can fix stuff" -- Richard Royal

Last edited by Paul Thompson; 03-16-2021 at 10:48 AM.
Reply With Quote
  #3  
Old 03-16-2021, 12:59 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,498
Pete VanderLaan is on a distinguished road
Why do these articles have to create such bad assertions.

"Other liquids, when cooled, more easily become glass. Silica, for example—window glass—starts as a molten liquid well above 1,000 degrees Celsius; as it cools, its disordered molecules contract slightly, crowding a bit closer together, which makes the liquid increasingly viscous. Eventually, the molecules stop moving altogether. In this gradual glass transition, the molecules don’t reorganize. They simply grind to a halt.
*********


This is just bullshit.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 03-16-2021, 02:50 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,026
Larry Cazes is on a distinguished road
Wired.com is NOT what I would call a credible source on Material Science
Reply With Quote
  #5  
Old 03-16-2021, 04:45 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,498
Pete VanderLaan is on a distinguished road
I think it potentially to be far more interesting is looking at why materials DO BECOME glass. Silica on it's own has a rough road. It needs modifiers to lower the temps to make the solutions possible and THEN it needs stabilizers to stop the action.
THEN, it need, under enormous pressure to be slow cooled so that the material just formed can have the huge pressure, measured in 1'000's of pls per sq inch pressure, relax so that the material formed is stable.

Comparing it to amber is just misguiding. They don't really have that much in common, besides clarity, a nice thing. I like fulgurites myself.

Your pissy management.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 03-16-2021, 08:16 PM
Brian Bradshaw Brian Bradshaw is offline
Registered User
 
Join Date: Jun 2016
Location: Lakewood, CA
Posts: 19
Brian Bradshaw is on a distinguished road
Doesn't anybody read Scholes anymore?
Reply With Quote
  #7  
Old 03-16-2021, 10:13 PM
David Hopman David Hopman is online now
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 447
David Hopman is on a distinguished road
The article is originally from Quanta magazine and reprinted by Wired.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:56 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.