Crucible schedule

I'm having problems searching this site at the moment.
Looking for ramp schedule for 300 lb crucible.
I remember a soak at 600c and again at 700c.
Any help appreciated.
TIA
Reply With Quote
  #2  
Old 03-22-2021, 08:02 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
I would advise ( selling pots) 50F per hr until you reach 1000F, then hold four hours, then 25 F for four hours to 1100F, hold four hours, then 50F until it starts to glow, then turn it up.

It's conservative but I prefer the safe side.

Much also depends on burner location, or if it's electric sitting on the floor. The heat stratification in electrics is worth paying a lot of attention to.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 03-22-2021, 12:28 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 619
Charles Friedman is on a distinguished road
Hi Tim Good to hear from you.
The best ramp schedule I have ever seen. Came from the genius Greg Englesby. "100 hours to 2000F degrees" one ramp. Pot empty or pot full. Seen it, done it, will not run anything else. Cheap insurance.

PS Give my regards to the lovely Tally.
__________________
"Glass will save the world from ourselfs" CharlesF

Last edited by Charles Friedman; 03-22-2021 at 12:32 PM.
Reply With Quote
  #4  
Old 03-22-2021, 03:10 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
pot full... I don't know why people do that. It's really hard on the pot.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-22-2021, 04:32 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 619
Charles Friedman is on a distinguished road
Sometimes shit happens and one has to startup where one lift off. Furnace crashes, pot full. Have done it a few times.
__________________
"Glass will save the world from ourselfs" CharlesF

Last edited by Charles Friedman; 03-22-2021 at 04:35 PM.
Reply With Quote
  #6  
Old 03-23-2021, 08:00 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
I was referring to putting a new pot in a kiln and then filling it with glass cullet and turning it on. That is really hard on a pot.

If it's a salvage operation, any port in a storm.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:55 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.