I will also add that the only way (just my opinion) that one can figure out how to make a solo studio work is to come up with a singular unique piece and then completely turn off your brain for the next 20 years and just keep making the same thing over and over.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #27  
Old 03-26-2021, 03:17 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 940
Michael Ahlefeldt-Laurvig is on a distinguished road
That can only be done with a large poupulation of very wealthy people
Reply With Quote
  #28  
Old 03-26-2021, 03:24 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Drone
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,274
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
...completely turn off your brain for the next 20 years...
I am unable to do this. It's the reason I never get anything done.
__________________
Temperature and time.
Reply With Quote
  #29  
Old 03-26-2021, 04:11 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,834
Eben Horton is on a distinguished road
Quote:
Originally Posted by greg vriethoff View Post
i am unable to do this. It's the reason i never get anything done.
oh look a squirrel !!!
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #30  
Old 03-26-2021, 05:41 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
It's two distinct methodologies. One is factory bases. One isn't . One seems to say if hands touched it while it went by, it's special, one doesn't. Essemce was based on this kind of tooling. Look at the video.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #31  
Old 03-26-2021, 05:42 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
That can only be done with a large poupulation of very wealthy people
***
and still is. The swedish approach is not at all cheap. They celebrate it.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #32  
Old 03-26-2021, 05:48 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
The business model of one person one piece died when the economy told it to die.

Very few people are able to do this completely solo, of if they are, there’s some serious family money to pad the losses.
****
I do it today for the same reasons I did it in 68. I prefer it. For me, I acknowledge the business aspect of it. I continue to celebrate the art despite it.


If it's money you want, it's really far easier to get it elsewhere.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #33  
Old 03-26-2021, 07:33 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,834
Eben Horton is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
****
I do it today for the same reasons I did it in 68. I prefer it. For me, I acknowledge the business aspect of it. I continue to celebrate the art despite it.


If it's money you want, it's really far easier to get it elsewhere.
I just want to blow glass
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #34  
Old 03-27-2021, 06:31 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
Says the video King.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #35  
Old 03-27-2021, 07:06 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,834
Eben Horton is on a distinguished road
My legacy. Hahah
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #36  
Old 03-27-2021, 09:23 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,578
Rich Samuel is on a distinguished road
Speaking of videos, where's our Peggy Guggenheim?

https://www.rottentomatoes.com/m/peg...eim_art_addict
Reply With Quote
  #37  
Old 03-27-2021, 09:43 AM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: Lakeland, Florida
Posts: 1,491
Tom Fuhrman is on a distinguished road
I see it this way,
There were 1000's of feet applied to stemware from 1900 to 1960 and there were all made with those 2 pieces of cherry wood put together with a strap. The old guys in WV and all thru the Midwest were able to do production of feet on multiple items with them all looking exactly the same.
Technology has come along and tried to replace craftsmanship and talent and in most instances it has but with it has come a lot of other factors that no one saw coming.
Reply With Quote
  #38  
Old 03-27-2021, 11:55 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Drone
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,274
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by eben horton View Post
oh look a squirrel !!!
Where!!! Where!!!
__________________
Temperature and time.
Reply With Quote
  #39  
Old 03-27-2021, 05:43 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 940
Michael Ahlefeldt-Laurvig is on a distinguished road
Quote:
Originally Posted by Tom Fuhrman View Post
I see it this way,
There were 1000's of feet applied to stemware from 1900 to 1960 and there were all made with those 2 pieces of cherry wood put together with a strap. The old guys in WV and all thru the Midwest were able to do production of feet on multiple items with them all looking exactly the same.
Technology has come along and tried to replace craftsmanship and talent and in most instances it has but with it has come a lot of other factors that no one saw coming.
Well yes Tom, but Im talking about the options today
Reply With Quote
  #40  
Old 03-28-2021, 08:36 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,499
Pete VanderLaan is on a distinguished road
W.va was really pre carbon availability. Shorty sent me mine in 76 and it was quite the thing at that time. If you compared the tooling for W.Va to the Essemce stuff, it was light years different. I think W.Va was far closer to the Carder/Tiffany era than to Sweden.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:53 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.