I'll take a stab at it.

I'm fascinated with old films of factories, especially glass. I think I missed my calling, and should have been an historian.

Anyway, I like this one of these Brits changing-out a monkey pot.

I think it's good to look back at how these things were done even if there are no longer any practical applications for the techniques. Who knows? You might get some ideas!
__________________
Temperature and time.
Reply With Quote
  #2  
Old 06-24-2015, 03:10 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Drone
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,274
Greg Vriethoff is on a distinguished road
Mold blowing and some rather interesting bit work. Even some cold working!
__________________
Temperature and time.
Reply With Quote
  #3  
Old 06-26-2015, 11:11 AM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,959
Dave Bross is on a distinguished road
I love the old ones too.

Here's Murano in the thirties:

https://www.youtube.com/watch?v=qxJs1Dh7_X4
__________________
Art is not a thing...it's a way.
Reply With Quote
  #4  
Old 01-08-2016, 02:35 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Drone
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,274
Greg Vriethoff is on a distinguished road
Glasfabriek Leerdam.

I like the handle touch down at 1:28. Someone taught me a variation of this technique once.

I don't speak Dutch, unfortunately.
__________________
Temperature and time.

Last edited by Greg Vriethoff; 01-08-2016 at 03:15 AM. Reason: clipboard fail
Reply With Quote
  #5  
Old 01-08-2016, 09:45 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Drone
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,274
Greg Vriethoff is on a distinguished road
This one has a groovy soundtrack. Dig the lab coat at 2:12.

Note the continued presence of tobacco. Wonder if the guy with the pipe might have taught Nick at one point.
__________________
Temperature and time.
Reply With Quote
  #6  
Old 09-29-2016, 11:49 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Drone
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,274
Greg Vriethoff is on a distinguished road
Since there's been some talk about the muff process on the board lately.
__________________
Temperature and time.
Reply With Quote
  #7  
Old 09-30-2016, 08:15 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,838
Eben Horton is on a distinguished road
Thanks for posting these Greg !
Reply With Quote
  #8  
Old 09-30-2016, 03:42 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,520
Pete VanderLaan is on a distinguished road
Adelle Pepper in "The glass Gaffers of New Jersey" has some great stuff on Muffs that were 6-8 feet tall. Those photos are in Finn Lyngaard's recipe book as well.

I have yet to really understand how they can bend windshield glass without leaving any marks. That's true of bent glass for showcases as well. I'd appreciate any enlightenment.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 09-30-2016, 04:02 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 1,029
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Adelle Pepper in "The glass Gaffers of New Jersey" has some great stuff on Muffs that were 6-8 feet tall. Those photos are in Finn Lyngaard's recipe book as well.

I have yet to really understand how they can bend windshield glass without leaving any marks. That's true of bent glass for showcases as well. I'd appreciate any enlightenment.
I bought a 6'x9' coffin kiln from a company that made curved panels for china cabinets and the like. It came with a mold in the bottom that bows up in the middle as you turn a crank from the outside. The crank arm has marks that gauge the amount of bow in the glass. It looks like the glass was suspended above the mold then as it starts to soften the mold is bowed up to lift the glass and let sag onto the mold. My guess was after it is bent they vent the kiln enough to freeze the glass and the mold is lowered. I removed it all from the kiln as it wasn't the direction I was going but it did make more questions then answers. A quick Google search revealed this company and its process.

http://youtu.be/HDR7kwPdiQg

How Do They Do It-- How Do They Make Curved Glass- Video at YourDiscovery.com.flv

I also just watched a process for windscreens but not nearly as impressive. As you can imagine that is very automated with time and temp repeated over and over and over.
Reply With Quote
  #10  
Old 09-30-2016, 06:43 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,578
Rich Samuel is on a distinguished road
In 1959, Steuben opened a new showroom on Fifth Ave. in NYC. Its front window was a huge concave quarter-round which made it look like there was no window at all. It must have cost a fortune, as I've only seen a similar, and much smaller, window one other time.

I can't believe I haven't found a picture of it online. In fact, the only picture I found was this one, which was taken late in Steuben's life, as they evidently replaced the (broken? failed?) glass with a flat pane some time after 1975, and the anti-skateboard/anti-homeless bars on the front bench help date it.
Attached Images
File Type: gif Steuben Window.gif (71.0 KB, 51 views)
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:01 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.