High temp metal pipe for gloryhole.

Looking for any help. I need a 3/4 pipe for my polite on my gloryhole. The stainless steel I have been getting can't handle the heat and crumbles. It need to be threaded on one side and at least 8" long 3/4 pipe that's 1.05 inches pipe. Thank you
Reply With Quote
  #2  
Old 01-28-2021, 07:48 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
This is a question with not enough information given. I dont have a clue what a polite is- but I do know its not a material issue , can you explain whats going on?
Reply With Quote
  #3  
Old 01-28-2021, 09:33 PM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 300
Chris Lowry is on a distinguished road
Pilot light?
Reply With Quote
  #4  
Old 01-28-2021, 09:50 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 619
Charles Friedman is on a distinguished road
Your pilot light is in the wrong spot.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #5  
Old 01-28-2021, 09:53 PM
Jesse Bogenrief Jesse Bogenrief is offline
Registered User
 
Join Date: Jun 2016
Location: Iowa
Posts: 22
Jesse Bogenrief is on a distinguished road
Sorry, yes pilot light. I have been trying to find Stainless steel T309 at least if not something like titanium.
Reply With Quote
  #6  
Old 01-29-2021, 08:01 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
You could just do away with it. A glory hole does not need a pilot light, its for like boilers and water heaters that cycle on and off to maintain a set temperature. Like I said its not a material issue- its a design flaw. Its not doing anything, and if it was its in the wrong place as Charles says.
It doesn't work as a safety valve either, glory holes are not prone to flame outs- if there was one the gas would reignite immediately because of the temperature in the hole, and the sensor would be way too slow to shut off the gas for the same reason.
If you wanted a safety shut down then it should be an optical flame sensor like you might have on as gas glass furnace.
Reply With Quote
  #7  
Old 01-29-2021, 09:15 AM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Watertown, MA
Posts: 156
Eric Trulson is on a distinguished road
Yeah, seconding what others have said, this is a design issue more than a material selection issue.

It's a good rule of thumb to just not have bare metal protruding into the hot interior of your gloryhole at all. Rapid oxidation is a hell of a drug, and even the high-temperature grades of stainless (309/310) won't like it for extended periods. Metals that would survive that environment happily are more like inconel and tungsten, and they're both expensive, hard to source, and troublesome to work. (although here's some inconel tube on mcmaster if you're a masochist)

Regular stainless pipe should survive much better as long as it's set an inch or two back into the wall (so assuming you have a brick interior on your GH, I'd have the tip of the metal pipe just poking an inch or less into the back side of the brick). Or as Michael says, unless you need the pilot light to adhere to code/insurance regs, you can ditch it entirely and just manually light the hole.

Last edited by Eric Trulson; 01-29-2021 at 09:17 AM.
Reply With Quote
  #8  
Old 01-29-2021, 10:24 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,515
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
You could just do away with it. A glory hole does not need a pilot light, its for like boilers and water heaters that cycle on and off to maintain a set temperature. Like I said its not a material issue- its a design flaw. Its not doing anything, and if it was its in the wrong place as Charles says.
It doesn't work as a safety valve either, glory holes are not prone to flame outs- if there was one the gas would reignite immediately because of the temperature in the hole, and the sensor would be way too slow to shut off the gas for the same reason.
If you wanted a safety shut down then it should be an optical flame sensor like you might have on as gas glass furnace.
*****
You may have a tough time getting that past many code inspectors. It falls into this notion of "Someone is always there". They actually go eat lunch among other things. I certainly agree that a gloryhole shutting off will spontaneously reignite. I use a variation of that premise on my furnace safety set up. The power will have to be out for at least 1/2 hour before the burner won't spontaneously reignite. Getting a gibberson style burner very far into the gloryhole is a great way to see how short the life on one of Gib's heads can be. It all depends on what you authority having jurisdiction says. I have no building code here at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 01-29-2021, 11:02 AM
Jesse Bogenrief Jesse Bogenrief is offline
Registered User
 
Join Date: Jun 2016
Location: Iowa
Posts: 22
Jesse Bogenrief is on a distinguished road
I must have pilot light and uv eye on all equipment for insurance and fire code. I'm in a building with over 100 other artists and non-profits organizations in downtown Des Moines Iowa.
Reply With Quote
  #10  
Old 01-29-2021, 11:29 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
Well yes I can understand the code thing- we used to have East Germany in Europe, Im just looking at it from a technical point.
Reply With Quote
  #11  
Old 01-29-2021, 12:38 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,515
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
Well yes I can understand the code thing- we used to have East Germany in Europe, Im just looking at it from a technical point.
****
At the beginning of the UBC and the UFC is a statement that this code may be altered at the discretion of the AHJ ( Auth having jurisdiction). It simply means if you can make a good case for a variance, the AHJ can accept it. They never do. The liability is pretty major despite the fact that we would all agree on how dumb it was.

I never did it but I can't recall anyone ever making a good argument for the variance. Even the gloryhole has strong arguments. If you've just lit it, it is not going to relight if it goes out, but it can pump gas, and will without supervision. I don't leave the area around my gloryhole until I know it's self sustaining. It's also a small shop.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 01-29-2021, 02:22 PM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 746
Art Freas is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
****
At the beginning of the UBC and the UFC is a statement that this code may be altered at the discretion of the AHJ ( Auth having jurisdiction). It simply means if you can make a good case for a variance, the AHJ can accept it. They never do. The liability is pretty major despite the fact that we would all agree on how dumb it was.

I never did it but I can't recall anyone ever making a good argument for the variance. Even the gloryhole has strong arguments. If you've just lit it, it is not going to relight if it goes out, but it can pump gas, and will without supervision. I don't leave the area around my gloryhole until I know it's self sustaining. It's also a small shop.
This is why I am pretty strict about having someone in the room at startup. Also I know if I replaced my glory holes I would not be able to use my current set up.
Reply With Quote
  #13  
Old 01-29-2021, 02:28 PM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 746
Art Freas is on a distinguished road
Also if you rent there is no way you can go without modern controls.
Reply With Quote
  #14  
Old 01-29-2021, 05:57 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,515
Pete VanderLaan is on a distinguished road
Actually Art, they're everywhere. It's more of a matter where you choose to set up shop.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #15  
Old 01-29-2021, 08:54 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
So this pipe goes to the front of your burner somehow and the tip is in the actual flame flow? And inside is the pilot sensor? What does it look like , how big is it and how far into the pipe does it sit? It is not being damaged at all? How long do you have to hold the start button when you light the burner? Does it ignite with a spark inside the pipe?
Can you take a picture that shows the arrangement?
Reply With Quote
  #16  
Old 01-29-2021, 09:25 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
Art, pilot light controllers Im guessing is 1920’s technique.
Anyway, you cant have unprotected metal in the glory, its not so much the temperature, its the atmosphere- both oxidation and reduction
I have no experience with inconel- but apparently is very resistant to atmosphere but has a service temp of 1200C. 2192f - thats not a happy glory hole
So if we have to go redneck fix with this design, we either have to protect the ss pipe or replace it
You guys think a thermo couple tube would take the thermo shock here?
Reply With Quote
  #17  
Old 01-30-2021, 08:36 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,837
Eben Horton is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
So this pipe goes to the front of your burner somehow and the tip is in the actual flame flow? And inside is the pilot sensor? What does it look like , how big is it and how far into the pipe does it sit? It is not being damaged at all? How long do you have to hold the start button when you light the burner? Does it ignite with a spark inside the pipe?
Can you take a picture that shows the arrangement?
Look at the website for The Ward power burner.
__________________
<EBEN EΠOIESEN >
Reply With Quote
  #18  
Old 01-31-2021, 10:39 PM
Ron Mynatt Ron Mynatt is offline
Registered User
 
Join Date: Apr 2008
Location: Springdale Arkansas
Posts: 169
Ron Mynatt is on a distinguished road
I would try inconel pipe, I put in inconel angle my furnace door and it works great.No scaling or deterioration of the metal.
Reply With Quote
  #19  
Old 02-02-2021, 01:41 PM
Mark Rendulic Mark Rendulic is offline
Registered User
 
Join Date: Aug 2015
Location: Austin Texas
Posts: 34
Mark Rendulic is on a distinguished road
Ever consider a ceramic tube like a thermocouple sleeve? That would take the heat better than any steel would.
Reply With Quote
  #20  
Old 02-10-2021, 08:44 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
Well Jesse seems not to be interested in fixing his problems, and Mark didnt read my post nor answered my question
Reply With Quote
  #21  
Old 02-11-2021, 07:10 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,515
Pete VanderLaan is on a distinguished road
Next they'll gossip about you on Reddit.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #22  
Old 02-12-2021, 06:55 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 944
Michael Ahlefeldt-Laurvig is on a distinguished road
Just bothers me a bit when newbies poke thier heads in and want instant gratifikation
Or suggest thinga without reading the threads
Careful, my covid 19 isolation is making me mean
Reply With Quote
  #23  
Old 02-13-2021, 07:00 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,515
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Michael Ahlefeldt-Laurvig View Post
Well Jesse seems not to be interested in fixing his problems, and Mark didnt read my post nor answered my question
****
A number of years back, there was this big fire in Seattle as I recall in one of those buildings where everything interconnected illegally. I'm sure someone could help me remember what that was. Then we had the guy who lit a full city block on fire trying to do blacksmith work after he was inspired by Forged in Fire.

I would have to agree that Code is based in Tragedy, not foresight.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #24  
Old 02-13-2021, 08:04 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,578
Rich Samuel is on a distinguished road
I don't recall that fire here, though it wouldn't surprise me if we had more than a few caused by ignorance. Are you thinking of the Ghost Ship fire in Oakland??

https://en.wikipedia.org/wiki/Ghost_...20of%20Oakland.
Reply With Quote
  #25  
Old 02-13-2021, 09:38 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,515
Pete VanderLaan is on a distinguished road
That sounds like it. I suppose I think of Seattle because of the rather remarkable building that the fish market is in. Pike Place? It would go up like a torch.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:14 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.