sodium volition

The last year was a blur for me in which I retreated entirely from making glass. The combination of Trump, turning 70, the COVID downturn had me leave the shop.
In that period of time, I never turned off my gas furnace which has a couple of color pots and the 75 lb clear, a pale ghost of how I once worked. It sat, always running, all this time as I rationalized my return. My first Vaccine was scheduled for today and I got it.

Yesterday, I made glass for the first time in all that time. The pot had been half full and it was indeed awkward to do it but I was OK. I'm only writing this to point out the workability of one year old molten glass.

It just about doesn't have any at all.

While it was not difficult to gather at 2085F, it showed itself after being on the punty. It had no fluidity at all. It was as short as Pittsburg plate glass I blew as a young man. You could grab it after a very hot reheat with tweezers and it barely budged. So, now, after the year, I'll throw it out and start over.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 03-09-2021, 06:34 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 753
Josh Bernbaum is on a distinguished road
Why keep the furnace running all that time?
Maybe that clear will be something that Kugler's opaque yellow finally fits.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass

Last edited by Josh Bernbaum; 03-09-2021 at 07:08 PM.
Reply With Quote
  #3  
Old 03-09-2021, 08:15 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,018
Hugh Jenkins is on a distinguished road
Pete, astounding to me that you would keep it running all that time, but I have to admit that the last year made usual life patterns disappear. We took eight months off from glass, the longest period in 52 years. It has taken time to get used to working again but it isn't the glass, its me. I have said before that I thought I was on my last crucible, but this time I'm pretty sure. I did a really nice melt last night and will keep playing on and off over the next year to see what life gives us after Trump and the Covid. Great not to be consumed by the daily Twitter reports, and somewhat relieved by having gotten the vaccine. I have enough batch for about 20 melts or so. Still get thinking about a miniature recuperation system sometimes. Why? Time will tell.
__________________
Aloha, Hugh
Reply With Quote
  #4  
Old 03-10-2021, 07:13 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,498
Pete VanderLaan is on a distinguished road
Days melted into the next day and time went by. I have the farm to care for, the issue of processing 15 cords of wood. A world in disease and a republican party that has gone totally mad leading us to pandemic. I had already purchased 5000 dollars worth of propane futures and so I never saw a bill as time went by.
As fall came on, freezing pipes were a concern and running was an easy fix. Dudley has a small furnace in his shop which serves the same purpose. By Oct, I was getting very inactive just waiting for the election, trnasfixed by the possibilities to come.

But that wasn't the point of this at all. It was the loss of viscosity. I was really impressed by how bad it could actually get. It looks great.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-10-2021, 07:44 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 940
Michael Ahlefeldt-Laurvig is on a distinguished road
So you have your thermo couple in the room and the setpoint on 70 right?
Reply With Quote
  #6  
Old 03-10-2021, 09:04 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,498
Pete VanderLaan is on a distinguished road
It's a warm thing in a sea of frozen things. It's not scientific... With it, the shop is at about 50F. The controllers won't work if it falls below 45F. They're really old, something like me. Some mornings, I flash a bernzomatic torch in the cabinet for them to wake them up. That works. Again not high tech. The diamond saw has an aquarium heater in the water to keep it unfrozen. The grinders really need hot water. I have fans by the furnace.

But that wasn't the point of this at all. It was the lack of viscosity he said, a second time.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 03-10-2021, 09:16 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is online now
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 940
Michael Ahlefeldt-Laurvig is on a distinguished road
So a new way to make boro glass then? Low temp.
Reply With Quote
  #8  
Old 03-10-2021, 12:04 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,498
Pete VanderLaan is on a distinguished road
That would be pretty extreme and somewhat slow but I do think I'll measure the linear expansion of the glass. Kind of like making Whisky. Three years in the pot, then finished on a blowpipe at the gloryhole. It needs an ad campaign.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:32 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.