pastoralli secrets needed

so can anyone help with sticking murrini on a ceramic pastorali please. i'm using a corundum plate and the murrini are sticking to the wash thats on the plate. i'm trying to get a full fuse/tack to roll up the glass onto a collar. i have kiln wash and bentonite available. i think there's too much wash on the plate first off. we heat and rotate the plate several times before the rollup. thoughts? vic
Reply With Quote
  #2  
Old 12-20-2017, 08:58 AM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,378
Eben Horton is on a distinguished road
15 years ago I bought some cast iron plates. Not once have I ever had a problem with sticking, spalling or anything. Ceramic plates get hot quick, are pourus and are brittle. The only upside I can see is that they are light.

That said. Have you tried ceramic paper? I think that is bomb proof, but dusty.
Reply With Quote
  #3  
Old 12-20-2017, 09:17 AM
Marty Kremer Marty Kremer is offline
Registered User
 
Join Date: May 2004
Location: North Yarmouth ME
Posts: 446
Marty Kremer is on a distinguished road
Have you tried Bullseye's kilnwash?
Reply With Quote
  #4  
Old 12-20-2017, 10:13 AM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 504
Art Freas is on a distinguished road
Most of the time sticking is because the wash was put on too thick. The wash should be really thin when put on, really thin, like watered down milk. And lots of coats.
Reply With Quote
  #5  
Old 12-20-2017, 11:05 AM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,861
David Patchen is on a distinguished road
Of course, there's lots of ways to skin this cat, but once you get it dialed, you'll rarely run into this problem again--until the plate needs re-washing. Here's blog post I did on this (since I get asked it a lot).

http://davidpatchen.com/content/how-...ne-and-murrine

Hope this helps. And keep your heats short!
Reply With Quote
  #6  
Old 12-20-2017, 11:58 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,504
Pete VanderLaan is on a distinguished road
Well written David. I have put a link to your site in Antiques and Classics on the subject unless you object. If so send Louis the Leg breaker to my winter quarters.

I will print it out if you don't mind, attribution of course.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 01:19 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.