Cork boards

ISO high density cork boards. I used to get mine from Gary, but that is not possible
Mine are 2" x 16" x 14". Anyone have some info they can share?
Thanks
Reply With Quote
  #2  
Old 12-29-2017, 10:59 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,013
Pete VanderLaan is on a distinguished road
I actually used to use ones from "Michael's" and they worked pretty well. Both David Patchen and Charlie Correll do have high density cork access.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 12-29-2017, 03:44 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,213
Eben Horton is on a distinguished road
I use yoga blocks.
Reply With Quote
  #4  
Old 12-29-2017, 04:59 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 934
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
I actually used to use ones from "Michael's" and they worked pretty well. Both David Patchen and Charlie Correll do have high density cork access.
Thanks, maybe one will chime in
The size I need is pretty big....
Reply With Quote
  #5  
Old 12-29-2017, 05:00 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 934
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
I use yoga blocks.
Too small ....
Reply With Quote
  #6  
Old 12-29-2017, 10:59 PM
Peter Bowles Peter Bowles is offline
Registered User
 
Join Date: Sep 2002
Location: Breadalbane, Tasmania
Posts: 612
Peter Bowles is on a distinguished road
I use cork floor tiles glued onto plywood - you can make them any size and shape you like. The cork is about 6mm thick I think. Works just fine.
Reply With Quote
  #7  
Old 12-29-2017, 11:12 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,835
David Patchen is on a distinguished road
Mark - let me know what size you need. I make my own cork paddles and cut from large thick sheets.
Reply With Quote
  #8  
Old 12-30-2017, 01:41 PM
Isaac Swanson Isaac Swanson is offline
Registered User
 
Join Date: Jun 2014
Location: Bainbridge island
Posts: 7
Isaac Swanson is on a distinguished road
Is there any reason that some cork insulation sheet wouldn’t work? Something like: https://www.mcmaster.com/#cork/=1awupoa
In the insulation section McMaster sells 4” thick cork sheets that are 12” x 36”
Reply With Quote
  #9  
Old 12-30-2017, 03:41 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 934
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Isaac Swanson View Post
Is there any reason that some cork insulation sheet wouldn’t work? Something like: https://www.mcmaster.com/#cork/=1awupoa
In the insulation section McMaster sells 4” thick cork sheets that are 12” x 36”
Its a density thing. My board has lasted over a year of hard use. There are many different types of cork...
Reply With Quote
  #10  
Old 12-30-2017, 03:43 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 934
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by David Patchen View Post
Mark - let me know what size you need. I make my own cork paddles and cut from large thick sheets.
Thanks David!
Mine are 2" thick x 16" x 14".... I'm trying to find out what I paid Gary for them...
Reply With Quote
  #11  
Old 12-30-2017, 07:41 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,835
David Patchen is on a distinguished road
Quote:
Originally Posted by Mark Rosenbaum View Post
Thanks David!
Mine are 2" thick x 16" x 14".... I'm trying to find out what I paid Gary for them...
I source monster blocks 24" x 36" x 4" that I cut down into paddle-sized pieces. I use high-density cork--the lower density stuff falls apart and burns up too easily. I've found that not only do they burn up at a different rate based on how you use them, but also how old the cork is. All things equal, recently manufactured cork seems to burn up a bit faster than older manufactured cork. New cork paddles with cork of any age seem to burn a bit quicker in the beginning, then settle down and are stable for years before they eventually burn out. Note that I always use them dry, not wet, so mine probably have a harder life. I probably get about 3 years out of a set of corks and I flatten 75% of my work.

Let me know if you'd like a 16 x 14 hunk of the high-density stuff.
Reply With Quote
  #12  
Old 12-31-2017, 02:32 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 185
David Russell is on a distinguished road
David I would be interested in a piece 12"x 12".... or larger if you prefer. How does that sound to you?
Reply With Quote
  #13  
Old 12-31-2017, 03:44 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,013
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by David Russell View Post
David I would be interested in a piece 12"x 12".... or larger if you prefer. How does that sound to you?
*******
Buy the whole piece...
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 12-31-2017, 04:12 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 934
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by David Patchen View Post
I source monster blocks 24" x 36" x 4" that I cut down into paddle-sized pieces. I use high-density cork--the lower density stuff falls apart and burns up too easily. I've found that not only do they burn up at a different rate based on how you use them, but also how old the cork is. All things equal, recently manufactured cork seems to burn up a bit faster than older manufactured cork. New cork paddles with cork of any age seem to burn a bit quicker in the beginning, then settle down and are stable for years before they eventually burn out. Note that I always use them dry, not wet, so mine probably have a harder life. I probably get about 3 years out of a set of corks and I flatten 75% of my work.

Let me know if you'd like a 16 x 14 hunk of the high-density stuff.
I'd love a hunk! Please email me ....info<at> rosetreegallery.com and we can do the transaction stuff! THANKS!
Reply With Quote
  #15  
Old 12-31-2017, 04:22 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,013
Pete VanderLaan is on a distinguished road
I have two paddles from David in that stuff and thy are very nice.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #16  
Old 12-31-2017, 04:25 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 185
David Russell is on a distinguished road
David, I would happily buy the 16" x14" piece if your willing to sell another. Your PM box is full.....
Reply With Quote
  #17  
Old 12-31-2017, 06:26 PM
David Patchen's Avatar
David Patchen David Patchen is offline
Registered User
 
Join Date: Sep 2005
Location: San Francisco, CA
Posts: 1,835
David Patchen is on a distinguished road
Quote:
Originally Posted by David Russell View Post
David, I would happily buy the 16" x14" piece if your willing to sell another. Your PM box is full.....
I'll quote you guys via email.

I wish the PM box was larger than 20! That's so 1996. I don't like putting my email out here because of spam bots but I'll find you guys...
Reply With Quote
  #18  
Old 12-31-2017, 07:04 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,013
Pete VanderLaan is on a distinguished road
If you put email in the cords seeds stones board, it is blocked from the google spider. I did that on purpose.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:56 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.