Reusable mold material

I'm slumping to about 1300 in an open faced mold with some detail but not crazy tight parameters. Looking for a reusable mold material rather than plater/silica. That option works fine except for the fragility of the mold after one firing. I didn't see much in the archive and Henry's book is in storage as Ive moved recently.
Anyone have experience with a refractory mold material?

Happy new year and thanks to Pete for keeping this forum up and running.
Reply With Quote
  #2  
Old 12-31-2017, 03:56 AM
Rosanna Gusler Rosanna Gusler is offline
Registered Fuser
 
Join Date: Mar 2003
Location: Wanchese, NC
Posts: 902
Rosanna Gusler is on a distinguished road
Ceramic clay, Kaiser Lee board , or rigidized ceramic fiber will all work.

Last edited by Rosanna Gusler; 12-31-2017 at 03:59 AM. Reason: More thought
Reply With Quote
  #3  
Old 01-01-2018, 01:34 PM
Gary Genetti Gary Genetti is online now
Registered User
 
Join Date: Feb 2017
Location: Hudson Valley, New York
Posts: 20
Gary Genetti is on a distinguished road
http://www.zrci.com/material/refract...pe-mold-mix-6/
http://www.zrci.com/material/rs-dd-sheet-types/
Mike Cauda at Zircar is good help.
mjcauda@zrci.com
Reply With Quote
  #4  
Old 01-02-2018, 07:08 AM
Jeffrey Mentuck Jeffrey Mentuck is offline
Registered User
 
Join Date: Mar 2016
Location: Salem
Posts: 13
Jeffrey Mentuck is on a distinguished road
If the detail is not too intricate, and there are no undercuts, a rigid sand mold made with sodium silicate can be good for a few burns.
Reply With Quote
  #5  
Old 01-02-2018, 05:44 PM
Andy Stenerson Andy Stenerson is offline
Registered User
 
Join Date: Aug 2007
Location: New York
Posts: 29
Andy Stenerson is on a distinguished road
Thank you all, I appreciate the info!
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:57 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.