I need a favor

Does anyone here have a thermjet tj-250 kicking around that I could borrow until august?

I just cracked mine and can't get a new one for a while. I guesss they are made to order ??? Crazy.


Here's hoping someone has one sitting on a shelf !
Reply With Quote
  #2  
Old 04-21-2017, 01:36 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 556
Charles Friedman is on a distinguished road
What part is cracked? If it is metal, use Marine tex. epoxy. If it is the refractory part contact Pryor Giggey and ask for there patching material.

http://www.pryorgiggey.com/
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #3  
Old 04-21-2017, 02:38 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
I think this burner is rebuildable but I am pressed for time due to orders.

I was hoping someone had a backup.
Reply With Quote
  #4  
Old 04-21-2017, 03:19 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 978
Mark Rosenbaum is on a distinguished road
I have a burner that I got from Wet Dog years and years ago (maybe 23 ). It was still functioning when I put in my moly furnace 11 years ago.... How can I tell if it is what you need?
Reply With Quote
  #5  
Old 04-21-2017, 05:07 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 88
Eric Trulson is on a distinguished road
Mark, the thermjet should have a sheet metal tag on it somewhere that lists some specs and a part number. Those part numbers usually follow the format "TJ-XXXX", where "XXXX" represents the maximum BTU/hr that burner is rated for.

Eben, if you aren't able to scare up a replacement burner and need to try to repair or patch your current one, I'd be happy to help. I've done a fair bit of work building glass equipment and am only a couple hours north of you.
Reply With Quote
  #6  
Old 04-23-2017, 09:51 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Thanks Eric !

I have located a loaner and will be picking it up this week, so I am all set, but thank you for the offer.
Reply With Quote
  #7  
Old 04-23-2017, 01:05 PM
Cecil McKenzie Cecil McKenzie is offline
Registered User
 
Join Date: Feb 2011
Location: Emporia, KS
Posts: 488
Cecil McKenzie is on a distinguished road
I was curious as to what cracked on the burner if you have time.? Thanks.
Reply With Quote
  #8  
Old 04-23-2017, 01:40 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 88
Eric Trulson is on a distinguished road
No problem Eben, hope you get hot again soon!

I'm curious about the cause/location of the crack myself, actually. I've installed a bunch of thermjets before, but have never had a chance to do regular maintenance or a swapout on one, so I'm not sure what their usual failure modes are.
Reply With Quote
  #9  
Old 04-23-2017, 01:46 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
The thermjet has a cast iron "nozzle" inside the ceramic tip. My burner's ceramic tip was cracked badly and the metal sheath had expanded and warped causing it to compress against the Mizzou burner block. When I tried to remove the burner from the block, the ceramic tip crumbled and the cast iron nozzle cracked in half. The burner is repairable but I chose to save that for another time when I have more time.

Last edited by Eben Horton; 04-23-2017 at 02:27 PM.
Reply With Quote
  #10  
Old 04-24-2017, 02:56 AM
Scott Benefield Scott Benefield is offline
Registered User
 
Join Date: Apr 2002
Location: Ballintoy, Northern Ireland
Posts: 86
Scott Benefield is on a distinguished road
Have you been running pre-heated combustion air through the Thermjet?
Reply With Quote
  #11  
Old 04-24-2017, 07:59 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Quote:
Originally Posted by Scott Benefield View Post
Have you been running pre-heated combustion air through the Thermjet?
Hi Scott!

Yes, but I had been monitoring the tempature of the air inlet pipe. It never went above 500 degrees.
Reply With Quote
  #12  
Old 04-24-2017, 08:03 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
The mistake I made was not packing the tip inside the burner block with ceramic fiber. I never knew that this had to be done. Because of this mistake, everything deteriorated over time.
Reply With Quote
  #13  
Old 04-25-2017, 03:08 AM
Scott Benefield Scott Benefield is offline
Registered User
 
Join Date: Apr 2002
Location: Ballintoy, Northern Ireland
Posts: 86
Scott Benefield is on a distinguished road
Eclipse makes a version of the Thermjet with a stainless spud (instead of malleable iron) for use with preheated combustion air. I think 500F is still too hot for their burner without that option.
Reply With Quote
  #14  
Old 04-25-2017, 10:58 AM
Andy Stenerson Andy Stenerson is offline
Registered User
 
Join Date: Aug 2007
Location: New York
Posts: 29
Andy Stenerson is on a distinguished road
Hey Eben, I think Scott is right about the stainless tip. Once I built my recuperator I swapped the iron for stainless and it's been trouble free. I have a thermjet 250 I'm not using but it's lacking the ceramic nozzle. Let me know if you're interested anyhow
Reply With Quote
  #15  
Old 04-25-2017, 03:20 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Thanks for the info guys.

i drove 4oo miles yesterday to obtain a loaner and now i have everything to get the furnace rebuilt and back up and running.

I will look into this stainless nozzle. Thanks!
Reply With Quote
  #16  
Old 04-25-2017, 03:34 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 990
Hugh Jenkins is on a distinguished road
I too have gotten stainless spuds made. I used to have to regularly change out the steel ones both for air and gas. They would actually start to leak around the orifice threads from expansion in the hot air stream or just corrosion. I need to get another set for the new small glory hole so if someone knows a place that would make several I would like to know. The ones i have were gifts made special when I was on the road doing installations.

They are not impossible to make using TOE (threaded one end) stainless nipples and taps and dies, but the wall thickness of the TOEs I get are not precise enough to always get good results.
__________________
Aloha, Hugh
Reply With Quote
  #17  
Old 04-25-2017, 05:08 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Hugh, do you use Thermjets with your recuperator systems??
Reply With Quote
  #18  
Old 04-25-2017, 05:57 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 990
Hugh Jenkins is on a distinguished road
No, Eben, I build the whole thing. My preheated air is in the 1200 to 1400 range. it travels through its own passages into the burner throat.
__________________
Aloha, Hugh
Reply With Quote
  #19  
Old 04-25-2017, 08:21 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Ok. That's what I thought!
Reply With Quote
  #20  
Old 04-26-2017, 03:58 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 512
Art Freas is on a distinguished road
Quote:
Originally Posted by Scott Benefield View Post
Eclipse makes a version of the Thermjet with a stainless spud (instead of malleable iron) for use with preheated combustion air. I think 500F is still too hot for their burner without that option.
look for the model number to have PCA in it.
Reply With Quote
  #21  
Old 04-26-2017, 05:02 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 990
Hugh Jenkins is on a distinguished road
Always have a spare.
__________________
Aloha, Hugh
Reply With Quote
  #22  
Old 04-26-2017, 05:18 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
What happens when that spud gets too hot inside the ceramic tip is that it expands against the tip and makes it crack. Also the stainless sleeve around the outside of the burner wants to expand and get all punky and warped. My sleeve expanded so much that it put outward forces on my burner block and made that crack and eventually crumble. John Chiles just told me that you have to pack fiber abound the thermjet tip to keep the sleeve from gettting too hot. I never knew that.
Reply With Quote
  #23  
Old 04-26-2017, 09:51 PM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 990
Hugh Jenkins is on a distinguished road
It can make a big difference too if you don't watch the gas/air ratio. Some excess air (15% air or 3% O2) works to help cool the burner parts but does not retard the combustion. I just don't like metal parts especially if exposed to back radiation from the fire box. Stainless has its life too, but it is longer.
__________________
Aloha, Hugh
Reply With Quote
  #24  
Old 04-27-2017, 02:51 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,753
Franklin Sankar is on a distinguished road
Eben if there is a space around the burner shouldn't it sucks air and keep the burner cooler??? If you put fiber it stops the air and what happens now?
Franklin
Reply With Quote
  #25  
Old 04-27-2017, 09:28 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,402
Eben Horton is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Eben if there is a space around the burner shouldn't it sucks air and keep the burner cooler??? If you put fiber it stops the air and what happens now?
Franklin
That logic works with a glory hole, but not with a furnace. I don't know why. Efficiency is my guess
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:53 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.