cullet.. ( the other kind)

For 20 years I have been tossing my cullet in the dumpster, but last week when I was at the dump I inquired about recycling the stuff.. ( pipe crack offs) and the answer was " absolutely ". So now I simply save my SP87 bags and fill them up with my scrap and recycle the whole thing. Every studio I know just pays to dispose of it..

Its my belief that all of the glass in my state gets ground up into fine frit and is used as road sand in the winter.

Just thought I would share...
__________________
<eben epoiese>
Reply With Quote
  #2  
Old 07-24-2018, 06:07 PM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Canal Fulton - Ohio
Posts: 495
Brian Graham is on a distinguished road
I sort mine - good clear gets saved for a future remelt. Colored bits get saved for a few artist friends - some even pay me good money for it. Fines below a 1/4", and super iron contaminated glass get pitched. I made a screen that goes over my trash bin for ease of sorting. I end up saving more glass than I throw away. I also run a two barrel system for crack offs - one for clear and one for color. This helps save time on the sort. I am going to ask my city if they would take what little I do throw out..... Never thought about recycling it till now.
__________________
The revolution will not be televised.

Last edited by Brian Graham; 07-24-2018 at 06:09 PM.
Reply With Quote
  #3  
Old 07-24-2018, 06:55 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,767
Pete VanderLaan is on a distinguished road
I save my moils to add to color, but never as a clear. The green is not acceptable.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-24-2018, 07:31 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,449
Eben Horton is on a distinguished road
Quote:
Originally Posted by Brian Graham View Post
I sort mine - good clear gets saved for a future remelt. Colored bits get saved for a few artist friends - some even pay me good money for it. Fines below a 1/4", and super iron contaminated glass get pitched. I made a screen that goes over my trash bin for ease of sorting. I end up saving more glass than I throw away. I also run a two barrel system for crack offs - one for clear and one for color. This helps save time on the sort. I am going to ask my city if they would take what little I do throw out..... Never thought about recycling it till now.
Oh yeah. I have a clear bucket and 2 color buckets. One wet and one dry. Saving clear saves me a lot of money over time.
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:11 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.