Double Checking on Cane Test

Quick question on cane testing.

You pull the pencil sized cane and put it directly in to the annealer, right? Or do you pull the cane and let it cool?
Reply With Quote
  #2  
Old 07-26-2018, 08:56 PM
Lawrence Tuber's Avatar
Lawrence Tuber Lawrence Tuber is offline
Registered User
 
Join Date: May 2011
Location: Columbus, OH
Posts: 23
Lawrence Tuber is on a distinguished road
I don't anneal pencil sized cane.. I make lots ..
Reply With Quote
  #3  
Old 07-26-2018, 09:03 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,565
Pete VanderLaan is on a distinguished road
what test are you trying to achieve?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-27-2018, 02:31 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 510
Art Freas is on a distinguished road
Your cane test with the pencil lead size between the bricks cantilevered out.
Reply With Quote
  #5  
Old 07-27-2018, 03:28 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,565
Pete VanderLaan is on a distinguished road
Ah, you posted pencil sized cane not pencil lead sized.

I can now assume you are checking your annealing temp. I pull and cool it. I don't care for being burned.

Pull some pencil lead diameter cane, around 4mm if that's clearer. Stick it between two bricks cantilevered out as suggested. Take the lehr up to 900F and after fifteen minutes, look at the cane. It still is straight, increase the temp to 925. Wash rinse repeat. Don't for get the fifteen minutes part . At a certain temp, that cane will slump hard. When it does, take 50F off of your control temp. That will give you a good notion of the upper range of the annealing range and remember it is a range. The hotter you can anneal, the faster the strain is relaxed. At the bottom end, the strain point is the point below which no further annealing can occur. From there on, you're trying to prevent thermal shock.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 07-28-2018, 03:42 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 510
Art Freas is on a distinguished road
Thanks much, appreciate the help!
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:16 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.