homemade unoxidized batch suggestions?

I'm interested in making an unoxidised batch, a 96, that has potassium, for melting sulfur/molybdenum ambers. Ive tried with our batch, East Bay regular, but the color doesn't take, I think because of the oxidizers. I know that SP sells a color base, and Im sure Jim would mix something for me but Id like to try myself.
I was going to start with Pete V's recipe of:
63.25 lbs sand
20.25 lbs soda ash
5.25 lbs potash
9.06 lbs hydrated lime
2.18 lbs 5 mole borax
Im considering upping the potash and decreasing the soda per and E&T's values but thought I'd see if any of you (perhaps Pete himself) had any suggestions.
Thanks in advance!
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:57 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.