corking molds

I got this as a private message and I don't yet have time to find the thread. Perhaps someone can do the simple search. It seems to me it was this:
http://talk.craftweb.com/showthread....=corking+molds
*****
Quote:
Originally Posted by pierre bowring
Hey how are you? I can’t seem to find the article Ed skeels wrote on corking steel molds. Also a guy I know told me Taylor kurle put a really good article up on corking steel molds with renite and can’t seem to find that either. Could you help me out? Finally, I know sorry this is a lot, I was curious if there was any info on mold blowing? Again have looked numerous times can’t seem to find anything. Thanks so much!
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #2  
Old 10-23-2019, 11:11 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
Not the thread but here's Mr. Wizard's instructions.
Reply With Quote
  #3  
Old 10-23-2019, 06:01 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 594
Charles Friedman is on a distinguished road
It helps to heat up the metal mold a little first, before adding the linseed. It helps with getting an even layer, let it drip upside down till it cools and gets real tacky, then apply the cork dust. And repeat 3 times.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #4  
Old 10-23-2019, 06:31 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,709
Jordan Kube is on a distinguished road
Forget the linseed oil. Use Renite. Ed switched to that.
__________________
WWUD? Think for yourself.
Reply With Quote
  #5  
Old 10-23-2019, 06:33 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,780
Eben Horton is on a distinguished road
I corked a 12 wides 32 cylinder mold with linseed oil. Dropped a bubble into it the first time and as I pulled the bubble out, the linseed oil vapors combusted and shot the bubble and pipe up about a foot in a giant cannon blast. Scared the crap out of me.
__________________
<eben epoiese>
Reply With Quote
  #6  
Old 10-27-2019, 12:00 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,239
Greg Vriethoff is on a distinguished road
Here
^^^^^^
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:25 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.