Sandblast resist

Anyone have a source for a nonpvc sandblast resist. I want to get some resist laser cut but I guess what I use wonít work.

Thanks
Reply With Quote
  #2  
Old 01-30-2018, 09:48 AM
Rick Wilton Rick Wilton is offline
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 188
Rick Wilton is on a distinguished road
not sure what you are using but ikonics makes a sandblast resist designed for laser engravers.

https://ikonicsimaging.com/mask-maki...lasertape.html

I use an either a photoresist or avery paint mask if I'm using my vinyl cutter.
Reply With Quote
  #3  
Old 01-30-2018, 12:24 PM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 248
Chris Lowry is on a distinguished road
Not sure I really understand this stuff.

I use Hartco products. I want to use a laser cutter to cut out patterns in the resist but I guess you donít want to use PVC based products.

I thought the ikonics product was for use in a laser ingraver but maybe Iím wrong.
Reply With Quote
  #4  
Old 01-30-2018, 01:05 PM
Rick Wilton Rick Wilton is offline
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 188
Rick Wilton is on a distinguished road
The link is for a laserable film. Your original post says you want some laser cut. There are four basic ways to create a sandblast mask.

Photoresist, laser, cutting plotter or handcut.

I currently do three of them and have done the laser in the past.

How fine of detail are you trying to achieve?
Reply With Quote
  #5  
Old 01-30-2018, 01:06 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 301
Steven O'Day is on a distinguished road
Laser engravers are the same as laser cutters but generally lower power. You do not want to use vinyl as it will gas off chlorine which corrodes the machine. I've had them cut 3m Buttercut, they were able to cut the stencil but leave the backing in place which helps hold together if there are a lot of small pieces.
Reply With Quote
  #6  
Old 01-30-2018, 01:19 PM
Rick Wilton Rick Wilton is offline
Registered User
 
Join Date: Oct 2005
Location: Calgary, Alberta Canada
Posts: 188
Rick Wilton is on a distinguished road
The vinyl I use through my knife cutting plotter is "avery paint mask" it is a low tack film so removes easily after blasting yet is strong enough that I can blast DEEP into the glass.
Reply With Quote
  #7  
Old 01-30-2018, 02:51 PM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 248
Chris Lowry is on a distinguished road
Yes I want to creat stencils by laser cut, not high detail just tiered of cutting it by hand. I really like the soft rubbery feel of the hartco products Iím using and I am doing medium depth blasting.

Maybe I should try the ikonics stuff.

Is Buttercut PVC free?
Reply With Quote
  #8  
Old 01-30-2018, 04:57 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,647
Jordan Kube is on a distinguished road
Why not use a plotter, Chris? They're pretty cheap.
__________________
WWUD? Think for yourself.
Reply With Quote
  #9  
Old 01-30-2018, 05:09 PM
Steven O'Day Steven O'Day is offline
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 301
Steven O'Day is on a distinguished road
The stencil part of buttercut is rubber, not sure about the backing part though
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:14 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.