lead cullet for sale

After over a year of searching I have finally found a source for lead cullet for casting.
If interested or know someone who is please call me at 804 334 8462.

Cost will most likely be in the $5 range. I am hoping to finalize the purchase in the next week or two.
Reply With Quote
  #2  
Old 01-31-2018, 04:09 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,553
Pete VanderLaan is on a distinguished road
Have you run a small sample cast yet? Lead is not necessarily the happiest of campers remelted.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 02-02-2018, 09:59 AM
neil duman neil duman is offline
Registered User
 
Join Date: May 2015
Location: VA
Posts: 15
neil duman is on a distinguished road
I'm picking up a sample and some formulas on Tuesday.

Will post results of the test casting.

I'm pretty optimistic after talking to the seller.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 02:38 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.