I have used tung oil for years. I started with it straight which works but takes a long time to dry. Pete is right. warming both the oil and glass first helps. Warm dry air circulation helps speed the drying. Curt Brock's lust'er product is tung oil with solvents. It works well and can be aplied in several coats to achieve desired finish. It does not store well and tends to jell in the can unless you use alot of it.
Reply With Quote
  #27  
Old 01-18-2018, 03:22 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
PotatoFish
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,007
Greg Vriethoff is on a distinguished road
To keep Liquid Lust'er from gelling in the can add marbles as you use it to displace the air. Leaving air in the can is what causes it to gel.

I believe this is in the directions on the package. I didn't come up with this myself.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #28  
Old 02-17-2018, 08:20 AM
Rich Arentzen Rich Arentzen is offline
Registered User
 
Join Date: Jun 2013
Location: Burlington, VT
Posts: 178
Rich Arentzen is on a distinguished road
Does the Luster yellow a bit over time?
Reply With Quote
  #29  
Old 02-17-2018, 11:33 AM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 248
Chris Lowry is on a distinguished road
My can of luster went bad over a year being opened only once. Seemed like a good product but expensive if your not using it all the time.
Reply With Quote
  #30  
Old 02-19-2018, 10:34 AM
Tony Serviente Tony Serviente is offline
Registered User
 
Join Date: Mar 2005
Location: Ithaca, NY
Posts: 155
Tony Serviente is on a distinguished road
For kiln work you can use a lead bearing overglaze, but it does not hold up to the weather and will craze and flake off over time. It also matures above the strain point so if the work is 3D it may move.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:34 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.