Door configuration for top of electric furnace

Which is better the flat door on top or the hood and a front door on the hood.
Franklin
Ps sorry about the sideways pic. It happens with iPad.
Attached Images
File Type: jpg 4764635D-DCD5-4988-BCED-E3BEED1F0ED0.jpg (26.5 KB, 42 views)
Reply With Quote
  #2  
Old 02-12-2018, 01:03 PM
Rick Kellner Rick Kellner is online now
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 137
Rick Kellner is on a distinguished road
Among many other factors, I imagine the 'answer' (for starters) is largely going to depend on whether or not the furnace is gas fired, or a wire melter. Then the size of the furnace would be the next thing I'd be considering.

I'm at a loss in thinking of many compelling reasons to have the crown and vertical door, if it is for smaller sized electric furnace. That might be more conducive to having enough space for efficient combustion in a gas furnace.

Maybe it's a philosophical question.
Reply With Quote
  #3  
Old 02-12-2018, 02:57 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,754
Franklin Sankar is on a distinguished road
Lol Rick. Yes it is electric. It works with the flat door on top except when you open the door I think lots of heat escapes . I was trying to trap some heat hence the attempt to make a hood over the port. Did not try it so cant give more info on what it will do. I expect the extra air space will increase the heat up time . Canít guess much more. It may be complete foolishness.
Franklin
Reply With Quote
  #4  
Old 02-12-2018, 03:19 PM
Eben Horton Eben Horton is online now
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,403
Eben Horton is on a distinguished road
If electric, go with the toilet seat door.
__________________
<eben epoiese>
Reply With Quote
  #5  
Old 02-12-2018, 03:34 PM
Rick Kellner Rick Kellner is online now
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 137
Rick Kellner is on a distinguished road
And the extra air space will add to operating expenses. Unless it's a furnace design (like a Denver) with elements up in the crown, that air space is also going to be far away from the bottom elements, and probably challenging to efficiently heat. The top elements are another can of worms altogether, and it seems like unnecessary complexity for perhaps no real gain.

What about thinking about a baffle in the lid, to trap heat in the firing chamber? Then you have the added benefit of minimizing element exposure to glass fumes while melting. Then when you flip open the door, the only primary mode of heat loss is going to be from the top opening of the crucible being exposed.
Reply With Quote
  #6  
Old 02-13-2018, 06:56 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,754
Franklin Sankar is on a distinguished road
Love the name Eben. Thanks Rick . I will work with the toilet seat and hope I donít end up with crap. Sorry could not resist that.
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:44 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.