Multiple gathers

Why do you make your second gather cover the entire first gather.?
Franklin
Reply With Quote
  #2  
Old 03-04-2019, 10:03 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,002
Mark Rosenbaum is on a distinguished road
So it is easier to keep an even bubble in your piece.... that is, if that is what you want
Reply With Quote
  #3  
Old 03-05-2019, 08:41 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,810
Franklin Sankar is on a distinguished road
Thanks. I want to cheat. As the glass in the pot gets used up I get to the point where it is not feasible. So I gather half way up and shape accordingly to make it even.
Franklin
Attached Images
File Type: jpg image.jpg (31.0 KB, 32 views)
Reply With Quote
  #4  
Old 03-05-2019, 08:57 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,767
Pete VanderLaan is on a distinguished road
use a round bottomed pot.

Further, not gathering completely over makes for a very difficult piece to neck down unless you have other design goals. Even further than that, the piece now has really different temperatures in it, some hot, some not so hot. I tend to think it makes progressing in skills difficult.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 03-05-2019, 10:39 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,810
Franklin Sankar is on a distinguished road
I knew somehow I could not get away with it . Did not realize it was so important.
If it should happen by accident (sometimes I miss the gathering mark) Can I save it if I heat the piece with uneven gathers ripping hot .
Franklin
Reply With Quote
  #6  
Old 03-05-2019, 11:09 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 905
Sky Campbell is on a distinguished road
I have a couple designs where I make my jack lines then post gather over half the piece roll in color and go.
Reply With Quote
  #7  
Old 03-05-2019, 11:42 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,449
Eben Horton is on a distinguished road
There are no rules Franklin! If you do things like this your work will look a lot different than a classically trained glassblower.
__________________
<eben epoiese>
Reply With Quote
  #8  
Old 03-05-2019, 12:00 PM
Eric Trulson Eric Trulson is online now
Young Turk
 
Join Date: Sep 2014
Location: Boston
Posts: 95
Eric Trulson is on a distinguished road
I feel your small-pot pain Franklin. My first furnace used 20lb pots that were designed for ladling steel in foundries. Tall & skinny, with a flat bottom.

When I got to the bottom of a pot and wasn't able to get full even gathers anymore, I had the most luck with just doing multiple small ugly gathers to get the total amount of glass I needed, then reheating everything (it's a looooooong reheat) and blocking to even out the form before blowing in the initial bubble. You're not going to make perfect pieces that way, but it lets you use up all your glass in the pot.
Reply With Quote
  #9  
Old 03-05-2019, 02:04 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,810
Franklin Sankar is on a distinguished road
Eric thanks , Itís nice to have someone who understand the woes of vertical gathering . I plan to pull cane or make marbles / paperweight when I reach the low limit.
Sky that is exactly what I try to do . Sometimes I loose the jackline but I heat up the neck in the burner flame and bring it back. I have to be careful I donít blow out the bottom but by gathering on the end helps with a thicker bottom.
Eben all I want to do is blow glass but I have to work with what I have for now. You make me so very curious with your answer.
Franklin
Reply With Quote
  #10  
Old 03-05-2019, 02:43 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,767
Pete VanderLaan is on a distinguished road
I think that it's fine to do things when you have a specific design goal in mind. That happens lots. On the other hand, doing things when you don't really recognize other options is maybe not quite so good.

Clearly to me, the main way one learns is by trying to duplicate work that one sees and admires. That allows you to measure yourself against a standard. The goal after that is learning to speak with your own voice and that's a lot harder.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #11  
Old 03-05-2019, 04:42 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,810
Franklin Sankar is on a distinguished road
I totally agree Pete but When I deviate Its because my limitations causing me to search for another way.
I hear you when you say glass remembers what you did to it so I expect trouble and that is why I ask all kinds of crazy questions. Its not that I donít want to do it like the teacher. I donít want to fix the unfixable, but I want to recognize the unfixable. It may take longer but for now I just want to box it.

Franklin
Reply With Quote
  #12  
Old 03-05-2019, 05:59 PM
Larry Cazes Larry Cazes is online now
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 891
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
I knew somehow I could not get away with it . Did not realize it was so important.
If it should happen by accident (sometimes I miss the gathering mark) Can I save it if I heat the piece with uneven gathers ripping hot .
Franklin
Nonsense. Dont count yourself out based on what others say until YOU know it to be so. Always question and experiment as much as possible.
Reply With Quote
  #13  
Old 03-05-2019, 06:32 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,810
Franklin Sankar is on a distinguished road
I try. Solving the punty problem will make all the difference.
Thanks
Franklin
Reply With Quote
  #14  
Old 03-05-2019, 07:27 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,002
Mark Rosenbaum is on a distinguished road
That being said, there are pieces that can be made by "posting up" a piece. Take your first gather and put a solid jack line in. Gather 1/2 way up and work the bottom/thicker glass as you normally would. Punty-up and open. This way, you can also get a thinner neck because it only has the thickness of the first gather.
Reply With Quote
  #15  
Old 03-06-2019, 07:52 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,810
Franklin Sankar is on a distinguished road
Mark you certainly know how to cheat. I note the jackline comes early. Do you blow it and put in the jackline with the first gather?
Thanks
Franklin
Reply With Quote
  #16  
Old 03-06-2019, 09:56 PM
Mark Rosenbaum's Avatar
Mark Rosenbaum Mark Rosenbaum is offline
Registered User
 
Join Date: Apr 2002
Location: New Orleans, LA
Posts: 1,002
Mark Rosenbaum is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Mark you certainly know how to cheat. I note the jackline comes early. Do you blow it and put in the jackline with the first gather?
Thanks
Franklin
Always blow out your bubble to an even desired thickness. With only one gather, you can go back with a good heat and put a jackline in..... p.s. it's not cheating if it works!
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:06 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.