Lap wheel

Does anyone out there have a lap wheel they are getting rid of?
I only need the wheel I can manage the stand, motor and such. I just want a second grit.
C
Reply With Quote
  #2  
Old 02-14-2018, 05:19 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
well, how flat, how big. I have a 38 inch not so flat that would make a nice coffee table. 1.29 " bore
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 02-14-2018, 06:23 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 942
Sky Campbell is on a distinguished road
Here's a option that worked for me and may be of interest to others.
Call your local bearing supplier and tell them you need a flat faced sprocket of whatever diameter you want. You can also buy the shaft, shaft collar, bearings and pulleys. If you looking for something in the 24" to 36" range it will be 2" thick or better. I found that to be the cheapest solution and they will pay the shipping. You of course need to be able to pick it up lol. I thought I would have to have them blanchard ground but to my surprise they are surfaced on a lathe and good enough for my needs.
Reply With Quote
  #4  
Old 02-15-2018, 02:41 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
If you can wait about 6 weeks I'm planning on getting some made if you want to jump in.
Reply With Quote
  #5  
Old 02-15-2018, 03:20 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
If you get surplus drops in larger machine shops, you'll get better price on the steel. If you buy a 4x7 sheet in 1.5 inch, it will cost you. I just bought what I found in surplus drop land. Sometimes 30 inch 1.5 inch. Sometimes 28 inch 3" thick. In my life I've worn through about six wheels down to too thin to true. I'd give you a 38 inch that can't be lathe ground. Too thin and it chatters. It could be run on a blanchard.

And max, I won't be here in July.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 02-16-2018, 11:06 AM
Chris Lowry Chris Lowry is offline
Registered User
 
Join Date: Oct 2003
Posts: 264
Chris Lowry is on a distinguished road
Max tell us more about a group buy
Reply With Quote
  #7  
Old 02-16-2018, 02:50 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
I am trying to imagine a worse idea than a group buy on wheel heads. Size alone will cause a crisis, thickness, then crating and shipping.. It is not a well thought through idea.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 02-16-2018, 04:35 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
It's probably cheaper to have them made yourself. Although I would be up for shipping and crating -- probably $250-350 for that alone.

I know where I can get some sizable drops (probably) for a decent price. Otherwise a fresh 24"x24" sheet 1.5" thick is $320 and weighs 244lbs.

I don't think there are any machine shops in town that can handle the job... other than the engineering school, which I have a good connection. They have a huge water jet also (probably 10'x20' just cool), if that would help in the process.

The fabrication lab at the National High Magnetic Field Laboratory down the street is also droolworthy.....

Pete is sending me a copy of the Hot Glass Info Exchange so I'll keep you updated on this journey

------

Note: I'll definitely be completing one first before I start taking orders!
Reply With Quote
  #9  
Old 02-16-2018, 05:01 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
24x 24? That,s not a sheet.

I was thinking a 4ft x 7 ft sheet of the same material. The only way you save a dime is to use the whole sheet, all at once. All processed the same so the lathe/ cutting tool set up needs no adjustments at all.

You're talking an expensive wheel.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 02-16-2018, 05:09 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
a 4 ft x 8 ft sheet is $1764. Which would make 12 two-foot wheels. Which would make each wheel about $150 or half the price of buying it cut ($320).

Trying to sell 12 wheels though, hah!

I bet I can get decent drops in the $200-250 range. They do a lot of bridges and steel-frame buildings. So getting them to cut up a big drop ain't no thang, they had some nice 2ft x 6 or 8ft last time I was there.
Reply With Quote
  #11  
Old 02-17-2018, 07:11 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
All the sheets I bought were 4x7 sheets which I always thought odd.
But have it clear faced ( machine shop speak) both sides, chamfered edge and center bored to 1.29.

You'll be a lot happier with a 30 inch wheel over a 24. My 38's were my favorites. That took a 2HP motor.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 03-12-2019, 11:46 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 230
Shawn Everette is on a distinguished road
If your still on the look hit up Glass Axis in Columbus OH. They had two sitting in the back collecting rust when I left. Know they want them gone., probably sell them for a song.
Reply With Quote
  #13  
Old 03-12-2019, 02:01 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
someone else perhaps. Even if you run diamonds, a thick head is what you want. Currently I have about a dozen wheelheads, more than my lifetime needs. . Thank you.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #14  
Old 03-16-2019, 12:03 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,679
Jordan Kube is on a distinguished road
Made a couple of similar wheels in December. This one is 37" across and 1.375" thick. Came in laser cut and blanchard ground. Just had to pop a hole big enough to get an endmill in to make the required size hole. Switched clamps and profiled the outside to finish. These were for the Ash Grove Cement plant in Seattle. I have no idea what they did with them. No I can't make them for people, better to buy local.
Attached Images
File Type: jpg Flat wheel blank resize.jpg (84.6 KB, 35 views)
File Type: jpg Flat wheel 1 resize.jpg (91.3 KB, 30 views)
File Type: jpg Flat wheel 2 resize.jpg (88.8 KB, 31 views)
File Type: jpg Flat wheel finish resize.jpg (91.8 KB, 32 views)
__________________
WWUD? Think for yourself.
Reply With Quote
  #15  
Old 03-16-2019, 07:21 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
locally, one will often find "drops" from heavy steel projects that are from 18-38 inch x 1.5 inch thick at local competent machine shops. They love selling them. Just have them clear faced both sides and chamfered with a center hole about .004 larger than your shaft. They do get heavy...

Nice work Jordan.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:35 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.