Goldilocks - move the punty

WRG finding a place to heat up the punty:

For certain, too cold is NOT OK.

Too hot, well, there are things to do about that - Simply pull the punty away from the heat. Of course, to far, and it will crack, to close and it slumps and makes a mess. But at least it's in your control.

You know it's too close when it moves.

The makeup of a "G-Punty" helps it be more robust:

- coat only the bottom 3/4" of the punty
- Very thin on the sides - maybe 1/16"
- About 1/8" on the bottom

This kind of punty can get relatively cool without cracking.

Monte
Reply With Quote
  #27  
Old 02-22-2019, 08:41 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Thanks for the dimensions it helps answer some questions. I have more glass on mine so when I heat it from the front of the GH and it gets ripping hot, the glass drips out. Hopefully the thinner layer of glass will not run off when it gets very hot. Itís easier to cool a hot punty than heat it up.
Eben if bill punty drives Lino crazy, I am mad for sure.
Franklin
Reply With Quote
  #28  
Old 02-22-2019, 11:09 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
Smile

Quote:
Originally Posted by Franklin Sankar View Post
Do you define the size of your punty by the size of the glass at the tapered end or the size/diameter of the pipe? I can vary the diameter of the end by tapering it.
Franklin
My measurements in mm were referring to the amount of glass off the pipe.

Build that rack! It will help you immensely. You could even cut a rectangle out of your glory door so you can slide the punties in there. Like Bill's.

You are definitely on track with the puntie you posted, except it is round, instead of flat at the tip.

And Bill would probably say you need to dip the iron or blow pipe half as deep. The glass on the puntie is too much. Your setup might prevent this however.

Looking good!

By the way, I kept butting heads with my girlfriend when she was learning Bill's technique from me. She kept wanting to skip steps, combine them etc. Follow the recipe for success
Reply With Quote
  #29  
Old 02-22-2019, 11:11 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
Another exercise Bill did was to practice gathering with a vat of honey. It has basically the same consistency as glass. That helped me out quite a bit.
Reply With Quote
  #30  
Old 02-22-2019, 03:01 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
the honey is a great idea for practice. I wasted well not wasted but use up lots of glass practicing and was doing the wrong thing over and over. I started out goodish and slowly lapsed into chaos. Back on track now.
Btw, honey is $100.00 for a bottle here. We not allowed to import honey.
So Michael hinted that I could use sugar and water. My GH is small. I welded a bracket to the door and welded rack on bracket.
Rack installed in front of door. see pics. The hole in the back did not work good. Too cold.
More testing tomorrow.
Franklin
Attached Images
File Type: jpg A5A282C3-996D-44D4-8DB1-CD45F2555CFC.jpg (51.7 KB, 30 views)
File Type: jpg C1ABABED-5CAA-42EB-8D3A-260E9EA97212.jpg (47.4 KB, 24 views)
File Type: jpg 5BCB43F8-26EF-4707-A6C8-082079D4ED6C.jpg (49.1 KB, 26 views)

Last edited by Franklin Sankar; 02-22-2019 at 03:04 PM.
Reply With Quote
  #31  
Old 02-22-2019, 04:33 PM
Ed Pennebaker's Avatar
Ed Pennebaker Ed Pennebaker is offline
Registered User
 
Join Date: Apr 2002
Location: Red Fern Glass near Green Forest, AR
Posts: 196
Ed Pennebaker is on a distinguished road
I reuse my punties most of the time. It stays about the right temp in the pipe warmer. Working alone I can keep the blowpipe in one hand, punty in the other, thirty seconds in the glory hole and they are ready to stick up.
Reply With Quote
  #32  
Old 02-22-2019, 05:44 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Thanks Ed. That is what we want to do. But by the time I heat up the punty pick up the piece from the hanger things start to fall apart. The timing and temp has to be precise.
So instead of heating up we cool down. This saves time for the Punty up and transfer.
Sounds easy . Ha. The next stage is to practice the punty up in one smooth motion. Accurate and spot on.
Franklin

Last edited by Franklin Sankar; 02-22-2019 at 05:47 PM.
Reply With Quote
  #33  
Old 02-22-2019, 07:31 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
Franklin: Part of the reality here is counter intuitive. Really small pieces are in fact a lot harder to make than bigger ones. It's just true.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #34  
Old 02-22-2019, 07:33 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Max Epstein View Post
Another exercise Bill did was to practice gathering with a vat of honey. It has basically the same consistency as glass. That helped me out quite a bit.
**
Steuben trained their new people on miscible oil/ Cold Molasses would work.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #35  
Old 02-22-2019, 10:18 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is offline
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 942
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
Franklin: Part of the reality here is counter intuitive. Really small pieces are in fact a lot harder to make than bigger ones. It's just true.
I think that's true in the beginning but my joints and muscles say otherwise. I have a hard time now with anything thick I can go thin even walled without thought but to make thick organic is just going against the grain.
Reply With Quote
  #36  
Old 02-22-2019, 11:58 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
**
Steuben trained their new people on miscible oil/ Cold Molasses would work.
I had to look up "miscible". One thought I had is -- why couldn't have Corning saved something, anything from Steuben in its new facility.


Franklin -- check this video out. It has a pretty good shot of the puntie coming out from the rack (an assistant certainly helps). It might take me a couple more days to find my videos.

https://www.youtube.com/watch?v=VizBKk2flY4
Reply With Quote
  #37  
Old 02-23-2019, 12:00 AM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
His assistant didn't bring the greatest one either.
Reply With Quote
  #38  
Old 02-23-2019, 12:50 AM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,454
Rich Samuel is on a distinguished road
It would be nice if they used noise-canceling microphones when they make these videos.
Reply With Quote
  #39  
Old 02-23-2019, 05:13 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Rich remember when we started on this board many years ago. I would have died for 5 minutes of video . Whitehouse had it all. Now they have disappeared and we have grown accustomed to numerous videos on YouTube.
They are the only ones I trust as not being fake. Oh sh... I hope they are real. With fake stories everyone looses.

Lifting the small pieces is certainly easier but starting with busting a hole with the punty on the bottom of the piece to all the other processes are torturous.
Franklin
Reply With Quote
  #40  
Old 02-23-2019, 05:31 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Just looked at the video Max. I can appreciate it more now. Thanks. Do you know if anything in his process changed from that time 2002.
Pete I was wondering why things were going good then after all these years it fell apart and I did not realize that I gradually creeped into making thin pieces.
Thanks for identifying it. Busting out a chunk from the bottom of a thick piece is no big thing. 😬
Franklin
Reply With Quote
  #41  
Old 02-23-2019, 07:12 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
[quote=Max Epstein;142875]I had to look up "miscible". One thought I had is -- why couldn't have Corning saved something, anything from Steuben in its new facility.?
QUOTE]
********
Lead. It pervaded the facility after all those years. I think the really big loss was the grinding and polishing equipment that was all remanded to the dump. It would be curious to know how they pulled that off. I don't have a clue as to where the mixing equipment went.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #42  
Old 02-23-2019, 07:18 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Just looked at the video Max. I can appreciate it more now. Thanks. Do you know if anything in his process changed from that time 2002.
Pete I was wondering why things were going good then after all these years it fell apart and I did not realize that I gradually creeped into making thin pieces.
Thanks for identifying it. Busting out a chunk from the bottom of a thick piece is no big thing. 😬
Franklin
******
Both small and small and thin lose heat really fast. The other issue there is how difficult it is to simply heat one part of a tiny piece. If it's under heated it puts enormous pressure on the punty when you try to tool it. From my point of view, if you are making things with two gathers or so that you should do what needs to be done before the glass loses its core heat. It works somewhat better in colored glass since that at least absorbs IR. Clear reflects it quite well.

If you have a good grinding shop, divots don't matter much. I don't do punties the way most people do anyways.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #43  
Old 02-23-2019, 07:20 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,104
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Rich remember when we started on this board many years ago. I would have died for 5 minutes of video . Whitehouse had it all. Now they have disappeared and we have grown accustomed to numerous videos on YouTube.
*****
Igneous glass bought up all the Whitehouse inventory. I don't have a clue what remains.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #44  
Old 02-25-2019, 10:23 PM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 726
Michael Ahlefeldt-Laurvig is on a distinguished road
Actually the oxygen/ gas torch did away with a lot of cold work, forget punties.
You can pick a stone or bubble right out of a comleted vase

Last edited by Michael Ahlefeldt-Laurvig; 02-25-2019 at 10:31 PM. Reason: Wrote wrong
Reply With Quote
  #45  
Old 03-02-2019, 08:10 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Anyone know that is the temperature in a pipe warmer.
Franklin
Reply With Quote
  #46  
Old 03-03-2019, 07:54 AM
Michael Ahlefeldt-Laurvig Michael Ahlefeldt-Laurvig is offline
Registered User
 
Join Date: Apr 2010
Location: Sweden
Posts: 726
Michael Ahlefeldt-Laurvig is on a distinguished road
Around 750C
Reply With Quote
  #47  
Old 03-03-2019, 08:44 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Thanks. 1382 f
Franklin
Reply With Quote
  #48  
Old 03-05-2019, 06:25 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Max I donít understand what you doing in your step 4. What thread? From pulling the glass out?
Thanks
Franklin
Reply With Quote
  #49  
Old 03-05-2019, 07:11 PM
Max Epstein Max Epstein is offline
Registered User
 
Join Date: Sep 2016
Location: Tallahassee, FL
Posts: 290
Max Epstein is on a distinguished road
Yes, from pulling the glass out, pull it back in toward your body so the thread wraps around the hot moile as you turn and the heat cuts it for you.

I haven't been able to get on my old phone with the videos... sorry
Reply With Quote
  #50  
Old 03-06-2019, 07:45 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,880
Franklin Sankar is on a distinguished road
Thanks Max. I am working a bit cold to cheat and get a bigger gather. but will have to increase the temp.
found some good videos on the Corning site.
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:37 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.