Originally Posted by Dan Vanantwerp View Post
10 lbs. My color crucibles are 17 lbs. I am able to get 6-8 lbs charged before my first blow session Saturday and then top off with the rest for Sunday.
*********
If you are using 10 lb mixes, if I understand that correctly, and you are adding around 300 grams of material to a mix you say Jim at East bay has already mixed, and you suggest it is mostly mixed by east bay, I think you're wrong. What I do think is that you're adding about 8% new materials to Jim's stuff in various semi hostile forms. In my mind, that''s a very large number. so, again, how are you mixing this new stuff in? What is your mixer?

Process is key in doing this stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #102  
Old 06-10-2018, 11:39 PM
Dan Vanantwerp Dan Vanantwerp is online now
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 222
Dan Vanantwerp is on a distinguished road
Success!

New recipe based on a 86.5 LEC worked perfectly for both the Cristalica AND Chalcedony glasses. Seems this stuff really wants a relatively low theoretical expansion to match a "96" glass just as Jordan suggested.

I performed the ring test with inside and outside applications. I was surprised enough when I opened the annealer to find everything intact. To pass the ring test with flying colors was hoped for, but really unexpected.

Going to repeat the formula in a larger scale and see if it passes a second analysis. Strangely, this mix seemed to strike a bit more quickly/easily than the previous mixes so I'll see if that remains consistent.

Pete, I'm doing my best to mix in a little food bucket I got at the restaurant supply store. They actually make a strainer that fits right on the top of it. I bought the lid and do some hard shaking, rolling and turning. I have thought of trying to secure it closed and place it in my cement mixer for a while. I've also used the drill mixer method but I don't think it's as thorough as what I've described.
__________________
My furnace setting: 2112
Reply With Quote
  #103  
Old 06-11-2018, 06:12 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,009
Pete VanderLaan is on a distinguished road
I am glad you are getting a fit. With the mixing you describe, I kind of doubt your results will be consistent. When I do a color additive using my clear that Spruce Pine mixed for me, in 14 lbs, adding seven grams, it goes back in the cement mixer for a half hour.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #104  
Old 06-12-2018, 02:50 PM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,928
Dave Bross is on a distinguished road
Get yourself a drill driven paint mixer, preferably plastic but steel works fine. The steel ones eventually eat up the bucket.

This will mix it up REALLY well and make you feel less like a performing monkey rolling a bucket around.

You can fabricate a dust cover for the bucket from plastic, cardboard, or whatever. The commercial ones look like a shower cap for someone with a head the size of a bucket and a hole dead center for the mixer shaft.

I just take it outside and wear a respirator and gloves.


https://www.homedepot.com/s/paint%2520mixer?NCNI-5
__________________
Art is not a thing...it's a way.

Last edited by Dave Bross; 06-12-2018 at 02:53 PM.
Reply With Quote
  #105  
Old Yesterday, 01:31 PM
Dan Vanantwerp Dan Vanantwerp is online now
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 222
Dan Vanantwerp is on a distinguished road
Confirmation

The results repeated with a new batch of Brossphate. Under my conditions, a theoretical expansion of 86.5 is the target. I've started making pieces with layers of Cristalica, Brossphate opal and Chalcedony with nice results. I'm about ready to try some colors, in addition to the white.

Just as Dave described, the glass can be made more opaque with additional reheats. It is worth taking an oxypropane torch to this glass to watch the waves of opacity form. I believe this is how Dave uses the glass and I didn't quite grasp what he was describing until I looked at it this way. With a torch and air gun (heat-cool cycles) the deep opacity can be coaxed out very easily. I was even able to get just a small section of the piece (the lip) to go deep opaque. Poor man's lip wrap
__________________
My furnace setting: 2112
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:35 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.