I've just put together a spread sheet for calculating L.E.C. (I know; its a guide not gospel) Is anyone willing to share any additional expansion values for things like strontium, or any other potentially useful ingredients, beyond what's listed in 'Modern Glass Practice' and 'Glass Notes IV'? Or have a suggestion of where to look for such additional values? Thanks in advance.
P.S. the original E&T values were published in 1927 in the Journal of the American Ceramic Society volume 10, pg. 551. It's a well written piece of history.
Reply With Quote
  #2  
Old 11-09-2019, 11:19 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,389
Pete VanderLaan is on a distinguished road
Look at Appen.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 11-09-2019, 10:15 PM
Josh Bernbaum Josh Bernbaum is offline
Registered User
 
Join Date: Feb 2009
Location: Brattleboro, VT
Posts: 736
Josh Bernbaum is on a distinguished road
I think Dave Bross mentioned here somewhere that strontium and barium were very similar on expansion factor. So I've been entering the strontium in the barium line of the spreadsheet. How accurate that is, I'm not sure yet but is what I've been doing on the spreadsheet for these phosphates I'm doing now which have a decent amt. of strontium.
__________________
www.jmbglass.com
instagram.com/joshbernbaum_glass
Reply With Quote
  #4  
Old 12-24-2020, 01:38 PM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,956
Dave Bross is on a distinguished road
Yup, what Josh said, I've got Barium at 1.40 and Strontium at 1.38.

One other you might not have, Phosphorous, P2O5, I have at .667

What's interesting to me is that as long as you're close, and you don't change the values for anything in the spreadsheet over time, your corrections getting to a match will take care of minor, and some major errors.

My opinion of the single most valuable aspect of a spreadsheet is in making those corrections to get a match with minimum tries.
__________________
Art is not a thing...it's a way.
Reply With Quote
  #5  
Old 12-24-2020, 04:25 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,389
Pete VanderLaan is on a distinguished road
that's interesting with the phosphate. It suggests a negative factor except that you can't just add P205. It needs to be attached to something which would throw the factor off. It is worth noting that calcium has a pretty low factor and that helps explain why one could add up to 5% cal phosphate without mismatch.

Of course then there are the ryolite stones.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 03-07-2021, 07:47 PM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,956
Dave Bross is on a distinguished road
I wrote it that way because the spreadsheet I made breaks every material into it's components then E&T factors each individual component.
__________________
Art is not a thing...it's a way.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:32 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.